Effects of trace C addition on the microstructure and refining efficiency of Al-Ti-B master alloy

被引:32
作者
Li, P. T. [1 ]
Ma, X. G. [1 ]
Li, Y. G. [1 ]
Nie, J. F. [1 ]
Liu, X. F. [1 ]
机构
[1] Shandong Univ, Key Lab Liquid Solid Struct Evolut & Proc Mat, Minist Educ, Jinan 250061, Peoples R China
关键词
Al-Ti-B master alloy; Grain refinement; TiC; TiB2; GRAIN-REFINEMENT; PERFORMANCE;
D O I
10.1016/j.jallcom.2010.04.251
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of a trace amount of C addition on the microstructure and refining performance of Al-Ti-B master alloy were studied and the Al-5Ti-0.8B-0.2C master alloy was prepared. Particles were extracted from the Al-5Ti-1B and Al-5Ti-0.8B-0.2C master alloys. In the Al-5Ti-1B master alloy, TiB2 particles exhibit hexagonal platelet and layered stacking morphologies, and agglomerate seriously in grain boundaries. After a trace amount of C is added, many paragenetic particles form in the Al-5Ti-0.8B-0.2C master alloy. They are composed of TiB2 particles and small TiC particles. The small TiC particles grow on the surface of TiB2 particles or are enchased in TiB2 particles. The existence of TiC particles weakens the TiB2 particle agglomerations obviously. Due to the microstructure improvement, the Al-5Ti-0.8B-0.2C master alloy shows much better refining performance than the Al-Ti-B master alloy. The average grain size of alpha-Al refined by 0.2 wt.% the prepared Al-5Ti-0.8B-0.2C master alloy is about 190 mu m. In addition, the refining efficiency of the Al-5Ti-0.8B-0.2C does not fade within 60 min. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:286 / 290
页数:5
相关论文
共 23 条
[1]   The influence of forming processes on the distribution and morphologies of TiC in Al-Ti-C master alloys [J].
Ding, Haimin ;
Liu, Xiangfa ;
Yu, Lina ;
Zhao, Guoqun .
SCRIPTA MATERIALIA, 2007, 57 (07) :575-578
[2]   A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles [J].
Easton, MA ;
StJohn, DH .
ACTA MATERIALIA, 2001, 49 (10) :1867-1878
[3]   Modelling of inoculation of metallic melts: Application to grain refinement of aluminium by Al-Ti-B [J].
Greer, AL ;
Bunn, AM ;
Tronche, A ;
Evans, PV ;
Bristow, DJ .
ACTA MATERIALIA, 2000, 48 (11) :2823-2835
[4]   Influence of high-intensity ultrasound on grain refining performance of Al-5Ti-1B master alloy on aluminium [J].
Han, YF ;
Li, K ;
Wang, J ;
Shu, D ;
Sun, BD .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 405 (1-2) :306-312
[5]  
JIANG WH, 1997, SPEC CAST NONFERROUS, V1, P19
[6]   Morphology Evolution of TiCx Grains During SHS in an Al-Ti-C System [J].
Jin, Shenbao ;
Shen, Ping ;
Zou, Binglin ;
Jiang, Qichuan .
CRYSTAL GROWTH & DESIGN, 2009, 9 (02) :646-649
[7]   Reaction tn Al-Ti-C powders and its relation to the formation and stability of TiC in Al at high temperatures [J].
Kennedy, AR ;
Weston, DP ;
Jones, MI ;
Enel, C .
SCRIPTA MATERIALIA, 2000, 42 (12) :1187-1192
[8]   Development of Al-5%Ti-1%B master alloy [J].
Krishnan, TS ;
Rajagopalan, PK ;
Gund, BR ;
Krishnan, J ;
Bose, DK .
JOURNAL OF ALLOYS AND COMPOUNDS, 1998, 269 (1-2) :138-140
[9]   Performance comparison of AlTiC and AlTiB master alloys in grain refinement of commercial and high purity aluminum [J].
Li, JG ;
Huang, M ;
Ma, M ;
Ye, W ;
Liu, DY ;
Song, DM ;
Bai, BZ ;
Fang, HS .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 (02) :242-253
[10]   Phase analysis of Al-Mn compounds in the AZ magnesium alloys [J].
Liu, Chuanpu ;
Pan, Fusheng ;
Wang, Weiqing .
2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 :395-+