B2O3 modified SiC-MoSi2 oxidation resistant coating for carbon/carbon composites by a two-step pack cementation

被引:86
作者
Fu, Qian-Gang [1 ]
Li, He-Jun [1 ]
Wang, Yong-Jie [1 ]
Li, Ke-Zhi [1 ]
Shi, Xiao-Hong [1 ]
机构
[1] NW Polytech Univ, CC Composites Res Ctr, Key Lab Ultrahigh Temp Composites, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Ceramic matrix composites; Intermetallic; Oxidation; CARBON-CARBON COMPOSITES; SI-MO; C/C COMPOSITES; PROTECTION;
D O I
10.1016/j.corsci.2009.06.033
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To protect carbon/carbon (C/C) composites against oxidation, a B2O3 modified SiC-MoSi2 coating was prepared by a two-step pack cementation. The microstructure and the oxidation resistant property of the coating were studied. The results show that, the as-received coating is a dense structure, and is composed of alpha-SiC, beta-SiC and MoSi2. The B2O3 modified SiC-MoSi2 coating has excellent oxidation resistant property, and can protect C/C composites from oxidation at 1773 K in air for more than 242 h. The failure of the coating was considered to arise from the existence of the penetration cracks in the coating during the slow cooling from 1873 to 673 K. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2450 / 2454
页数:5
相关论文
共 21 条
[1]   A Si-Mo fused slurry coating for oxidation protection of carbon-carbon composites [J].
Fang, HT ;
Zhu, JC ;
Yin, ZD ;
Jeon, JH ;
Hahn, YD .
JOURNAL OF MATERIALS SCIENCE LETTERS, 2001, 20 (02) :175-177
[2]   Mullite based oxidation protection for SiC-C/C composites in air at temperatures up to 1900 K [J].
Fritze, H ;
Jojic, J ;
Witke, T ;
Rüscher, C ;
Weber, S ;
Scherrer, S ;
Weiss, R ;
Schultrich, B ;
Borchardt, G .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (16) :2351-2364
[3]   Silicide coating for protection of C/C composites at 1873 K [J].
Fu Qian-Gang ;
Li He-Jun ;
Shi Xiao-Hong ;
Li Ke-Zhi ;
Huang Min ;
Sun Guo-Dong .
SURFACE & COATINGS TECHNOLOGY, 2006, 201 (06) :3082-3086
[4]   SiC whisker-toughened MoSi2-SiC-Si coating to protect carbon/carbon composites against oxidation [J].
Fu Qian-Gang ;
Li He-Jun ;
Li Ke-Zhi ;
Shi Xiao-Hong ;
Hu Zhi-Biao ;
Huang Min .
CARBON, 2006, 44 (09) :1866-1869
[5]   RAPID DENSIFICATION OF POROUS CARBON-CARBON COMPOSITES BY THERMAL-GRADIENT CHEMICAL-VAPOR INFILTRATION [J].
GOLECKI, I ;
MORRIS, RC ;
NARASIMHAN, D ;
CLEMENTS, N .
APPLIED PHYSICS LETTERS, 1995, 66 (18) :2334-2336
[6]   Preparation and oxidation kinetics mechanism of three-layer multi-layer-coatings-coated carbon/carbon composites [J].
Huang, JF ;
Li, HJ ;
Zeng, XR ;
Li, KZ .
SURFACE & COATINGS TECHNOLOGY, 2006, 200 (18-19) :5379-5385
[7]   Oxidation through coating cracks of SiC-protected carbon/carbon [J].
Jacobson, Nathan S. ;
Roth, Don J. ;
Rauser, Richard W. ;
Cawley, James D. ;
Curry, Donald M. .
SURFACE & COATINGS TECHNOLOGY, 2008, 203 (3-4) :372-383
[8]   Oxidation microstructure studies of reinforced carbon/carbon [J].
Jacobson, NS ;
Curry, DM .
CARBON, 2006, 44 (07) :1142-1150
[9]   SiC-MoSi2-(Ti0.8Mo0.2)Si2 multi-composition coating for carbon/carbon composites [J].
Jiao, Geng-sheng ;
Li, He-jun ;
Li, Ke-zhi ;
Wang, Chuang ;
Hou, Dang-she .
SURFACE & COATINGS TECHNOLOGY, 2006, 201 (06) :3452-3456
[10]   A MoSi2-SiC-Si oxidation protective coating for carbon/carbon composites [J].
Li, He-Jun ;
Xue, Hui ;
Wang, Yong-Jie ;
Fu, Qian-Gang ;
Yao, Dong-Jia .
SURFACE & COATINGS TECHNOLOGY, 2007, 201 (24) :9444-9447