Three-Phase 3D Reconstruction of a LiCoO2 Cathode via FIB-SEM Tomography

被引:41
作者
Liu, Zhao [1 ]
Chen-Wiegart, Yu-chen K. [2 ]
Wang, Jun [2 ]
Barnett, Scott A. [1 ]
Faber, Katherine T. [1 ,3 ]
机构
[1] Northwestern Univ, Dept Mat Sci & Engn, Evanston, IL 60208 USA
[2] Brookhaven Natl Lab, Photon Sci Directorate, Upton, NY 11973 USA
[3] CALTECH, MC 138-78, Pasadena, CA 91125 USA
关键词
Li-ion batteries; three-phase 3D reconstruction; FIB-SEM tomography; cathode; microstructure; 3-DIMENSIONAL MICROSTRUCTURE; ELECTRON-MICROSCOPY; ION; TORTUOSITY; VISUALIZATION; ENERGY;
D O I
10.1017/S1431927615015640
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Three-phase three-dimensional (3D) microstructural reconstructions of lithium-ion battery electrodes are critical input for 3D simulations of electrode lithiation/delithiation, which provide a detailed understanding of battery operation. In this report, 3D images of a LiCoO2 electrode are achieved using focused ion beam-scanning electron microscopy (FIB-SEM), with clear contrast among the three phases: LiCoO2 particles, carbonaceous phases (carbon and binder) and the electrolyte space. The good contrast was achieved by utilizing an improved FIB-SEM sample preparation method that combined infiltration of the electrolyte space with a low-viscosity silicone resin and triple ion-beam polishing. Morphological parameters quantified include phase volume fraction, surface area, feature size distribution, connectivity, and tortuosity. Electrolyte tortuosity was determined using two different geometric calculations that were in good agreement. The electrolyte tortuosity distribution versus position within the electrode was found to be highly inhomogeneous; this will lead to inhomogeneous electrode lithiation/delithiation at high C-rates that could potentially cause battery degradation.
引用
收藏
页码:140 / 148
页数:9
相关论文
共 36 条
[1]  
Abrmoff MD., 2004, Image Processing with ImageJ, V11, P36, DOI DOI 10.1201/9781420005615.AX4
[2]   Multiple imaging mode X-ray computed tomography for distinguishing active and inactive phases in lithium-ion battery cathodes [J].
Babu, Siddharth Komini ;
Mohamed, Alexander I. ;
Whitacre, Jay F. ;
Litster, Shawn .
JOURNAL OF POWER SOURCES, 2015, 283 :314-319
[3]   Tortuosity characterization of 3D microstructure at nano-scale for energy storage and conversion materials [J].
Chen-Wiegart, Yu-chen Karen ;
DeMike, Ross ;
Erdonmez, Can ;
Thornton, Katsuyo ;
Barnett, Scott A. ;
Wang, Jun .
JOURNAL OF POWER SOURCES, 2014, 249 :349-356
[4]   3D analysis of a LiCoO2-Li(Ni1/3Mn1/3Co1/3)O2 Li-ion battery positive electrode using x-ray nano-tomography [J].
Chen-Wiegart, Yu-chen Karen ;
Liu, Zhao ;
Faber, Katherine T. ;
Barnett, Scott A. ;
Wang, Jun .
ELECTROCHEMISTRY COMMUNICATIONS, 2013, 28 :127-130
[5]   Image based modelling of microstructural heterogeneity in LiFePO4 electrodes for Li-ion batteries [J].
Cooper, S. J. ;
Eastwood, D. S. ;
Gelb, J. ;
Damblanc, G. ;
Brett, D. J. L. ;
Bradley, R. S. ;
Withers, P. J. ;
Lee, P. D. ;
Marquis, A. J. ;
Brandon, N. P. ;
Shearing, P. R. .
JOURNAL OF POWER SOURCES, 2014, 247 :1033-1039
[6]  
Dijkstra EW., 1959, NUMER MATH, V1, P269, DOI 10.1007/BF01386390
[7]   MODELING OF GALVANOSTATIC CHARGE AND DISCHARGE OF THE LITHIUM POLYMER INSERTION CELL [J].
DOYLE, M ;
FULLER, TF ;
NEWMAN, J .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (06) :1526-1533
[8]   THE USE OF MATHEMATICAL-MODELING IN THE DESIGN OF LITHIUM POLYMER BATTERY SYSTEMS [J].
DOYLE, M ;
NEWMAN, J .
ELECTROCHIMICA ACTA, 1995, 40 (13-14) :2191-2196
[9]   Tortuosity Anisotropy in Lithium-Ion Battery Electrodes [J].
Ebner, Martin ;
Chung, Ding-Wen ;
Garcia, R. Edwin ;
Wood, Vanessa .
ADVANCED ENERGY MATERIALS, 2014, 4 (05)
[10]   Visualization and Quantification of Electrochemical and Mechanical Degradation in Li Ion Batteries [J].
Ebner, Martin ;
Marone, Federica ;
Stampanoni, Marco ;
Wood, Vanessa .
SCIENCE, 2013, 342 (6159) :716-720