Bi2-xSbxTe3-ySey (x = 0.1, 0.2 and y = 0.15, 0.3) solid solutions were prepared using encapsulated melting and hot pressing. The lattice constants decreased with increases in the Sb and the Se contents, which revealed the successful formation of solid solutions. The relative densities of the hot-pressed specimens were 95-98%. All specimens exhibited n-type conduction at temperatures from 323 K to 523 K, and the electrical conductivity slightly decreased with increasing temperature. With an increase in the Se content, the Seebeck coefficient increased while the electrical and the thermal conductivities decreased; thus, the dimensionless figure of merit could be improved. The maximum dimensionless figure of merit ZTmax = 0.89 was obtained at 423 K for Bi1.8Sb0.2Te2.7Se0.3. An increase in the Sb content resulted in a decrease in the lattice thermal conductivity because of an increase in alloy scattering, but its effect on the electrical properties was not superior to the effect of Se substitution. Therefore, Sb substitution could effectively control the thermal properties while Se substitution could effectively control the electrical properties.
引用
收藏
页码:505 / 510
页数:6
相关论文
共 29 条
[1]   Cooling, heating, generating power, and recovering waste heat with thermoelectric systems [J].
Bell, Lon E. .
SCIENCE, 2008, 321 (5895) :1457-1461
[2]   Properties and Formation of the Structure of Bi2Se0.3Te2.7 Solid Solutions Produced by Equal-Channel Angular Pressing [J].
Bogomolov, D. I. ;
Bublik, V. T. ;
Tabachkova, N. Yu. ;
Tarasova, I. V. .
JOURNAL OF ELECTRONIC MATERIALS, 2016, 45 (01) :403-410
[3]   Nanostructured materials for thermoelectric applications [J].
Bux, Sabah K. ;
Fleurial, Jean-Pierre ;
Kaner, Richard B. .
CHEMICAL COMMUNICATIONS, 2010, 46 (44) :8311-8324
[4]   Properties of single crystalline semiconducting CoSb3 [J].
Caillat, T ;
Borshchevsky, A ;
Fleurial, JP .
JOURNAL OF APPLIED PHYSICS, 1996, 80 (08) :4442-4449
[5]   ATOMIC SCREENING CONSTANTS FROM SCF FUNCTIONS .2. ATOMS WITH 37 TO 86 ELECTRONS [J].
CLEMENTI, E ;
RAIMONDI, DL ;
REINHARDT, WP .
JOURNAL OF CHEMICAL PHYSICS, 1967, 47 (04) :1300-+
[6]   CHEMICAL BONDING IN BISMUTH TELLURIDE [J].
DRABBLE, JR ;
GOODMAN, CHL .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1958, 5 (1-2) :142-144
[7]   p-type Bi0.4Sb1.6Te3 nanocomposites with enhanced figure of merit [J].
Fan, Shufen ;
Zhao, Junnan ;
Guo, Jun ;
Yan, Qingyu ;
Ma, Jan ;
Hng, Huey Hoon .
APPLIED PHYSICS LETTERS, 2010, 96 (18)
[8]   Comparative studies between the growth characteristics of Bi2Te3 thin films deposited on SiO2, Si(100) and Si(111) [J].
Ferhat, M ;
Liautard, B ;
Brun, G ;
Tedenac, JC ;
Nouaoura, M ;
Lassabatere, L .
JOURNAL OF CRYSTAL GROWTH, 1996, 167 (1-2) :122-128
[9]  
Goldsmid HJ, 1964, THERMOELECTRIC REFRI, P43
[10]   Enhancement in thermoelectric performance of bismuth telluride based alloys by multi-scale microstructural effects [J].
Hu, Lipeng ;
Gao, Hongli ;
Liu, Xiaohua ;
Xie, Hanhui ;
Shen, Junjie ;
Zhu, Tiejun ;
Zhao, Xinbing .
JOURNAL OF MATERIALS CHEMISTRY, 2012, 22 (32) :16484-16490