Behavior of Short-Span Concrete Members Internally Reinforced with Glass Fiber-Reinforced Polymer Bars

被引:15
作者
Abu-Obaida, Ayman [1 ]
El-Ariss, Bilal [1 ]
El-Maaddawy, Tamer [1 ]
机构
[1] United Arab Emirates Univ, Dept Civil & Environm Engn, POB 15551, Al Ain, U Arab Emirates
关键词
Short span; Glass fiber-reinforced polymer (GFRP) reinforcement; Shear strength; Strut-and-tie method; SHEAR-STRENGTH; WEB REINFORCEMENT; DEEP BEAMS; STIRRUPS; CORBELS;
D O I
10.1061/(ASCE)CC.1943-5614.0000877
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper aims to investigate the behavior of short-span concrete members with a shear span-to-effective depth ratio (a/d) less than 2, internally reinforced with glass fiber-reinforced polymer (GFRP) bars. The study comprised testing of 12 specimens. Test parameters included the a/d ratio, GFRP reinforcement ratio, and concrete grade. The study was supplemented by an analytical investigation to predict the strength of the tested specimens. The experimental study highlighted that increasing the longitudinal GFRP reinforcement ratio together with the concrete strength in the absence of web reinforcement might be detrimental to the strength of GFRP-reinforced short-span concrete members due to a shift in the mode of failure from crushing of a diagonal strut to diagonal splitting. Experimental results indicate also that increasing the a/d does not necessarily reduce the strength of short-span GFRP-reinforced concrete specimens with a low concrete strength due to a greater angle of inclination of the critical shear crack developed during testing relative to that considered in the analysis. The strut-and-tie modeling (STM) provided conservative predictions for the nominal strength of the tested specimens except for those failed by diagonal splitting where it overestimated the strength by a maximum of 12%. The accuracy and validity of two published analytical approaches were examined. These approaches tended to provide less conservative, yet reasonable, nominal strength predictions but overestimated the strength of the specimens with the diagonal splitting mode of failure.
引用
收藏
页数:11
相关论文
共 25 条
  • [1] Shear characteristics of GFRP-reinforced concrete deep beams without web reinforcement
    Abed, F.
    El-Chabib, H.
    AlHamaydeh, M.
    [J]. JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2012, 31 (16) : 1063 - 1073
  • [2] Andermatt MF, 2013, ACI STRUCT J, V110, P595
  • [3] [Anonymous], 2008, Building Code Requirements for Structural Concrete (ACI 318-08)
  • [4] [Anonymous], 2015, ACI-440.1R-15
  • [5] [Anonymous], 2012, ACI 440.3R-12.
  • [6] Shear Strength of Large Concrete Members with FRP Reinforcement
    Bentz, Evan C.
    Massam, Laurent
    Collins, Michael P.
    [J]. JOURNAL OF COMPOSITES FOR CONSTRUCTION, 2010, 14 (06) : 637 - 646
  • [7] Carnpione G, 2007, ACI STRUCT J, V104, P570
  • [8] CSA (Canadian Standard Association), 2012, S806 CSA CAN
  • [9] Concrete Contribution to Shear Strength of Beams Reinforced with Basalt Fiber-Reinforced Bars
    El Refai, Ahmed
    Abed, Farid
    [J]. JOURNAL OF COMPOSITES FOR CONSTRUCTION, 2016, 20 (04)
  • [10] El-Sayed AK, 2006, ACI STRUCT J, V103, P235