摘要
Purposes (1) To evaluate different pre-treatment modes for partial resin-based composite repair using a shear bond strength fatigue design on aged specimens, and (2) to investigate the effect of these pre-treatments on aged and partially replaced Class II resin-based composite restorations. Materials and Methods: (Study 1) 150 composite discs (Tetric Ceram) were light-cured, secondary cured, and stored in water for 365 days. The specimens were randomly assigned to five pretreatment groups (n=30): (1) Roughening with a finishing diamond bur + dentin bonding system (DBS, Syntac Classic), (2) Roughening with a silicon carbide bur + DBS, (3) Roughening with a silicon carbide bur + DBS + Tetric Flow, (4) silica-coating (CoJet) + DBS, and (5) silica-coating + dentin bonding agent + Tetric Flow. The disks were restored with fresh repair composite cylinders and after 24-hour water storage, initial bond strengths (n=10) and fatigue bond strengths (n=20; 5,000 cycles in shear mode) were evaluated and fracture modes determined under a SEM. (Study 2): 40 Class II restorations (EBS Multi/Pertac II) were placed in extracted human third molars. The specimens were stored for 365 days and then replaced partially by removing the proximal box and leaving the occlusal part. The partial repairs (Pertac 11) were placed after identical pre-treatment modes A-E (n=8). After thermomechanical loading (100,000 x 50 N, simultaneously x2,500 at 5degreesC/55degreesC), marginal quality between old and fresh composite was evaluated by SEM at x200 magnification and dye penetration was observed by light microscopy under x50 magnification. Results: Initial repair bond strengths were significantly higher for the groups with additional application of flowable composite compared to composite only (P< 0.05; Mann Whitney U test). Diamond finishing revealed the lowest bond strengths. Fatigue bond strengths exhibited the worst results for Group 1 as well, but were similar for Groups 2-5. In the Class II partial repair simulation, Groups 3 and 5 with additional flowable lining exhibited significantly better marginal quality and significantly lower leakage, whereas the other groups revealed up to 100% separation between aged and freshly applied composite. (Am J Dent 2003; 16:17-22).
引用
收藏
页码:17 / 22
页数:6
相关论文
共 50 条
  • [31] Bond strength of resin-based restorations polymerized with different light-curing sources
    D'Alpino, Paulo H. P.
    Wang, Linda
    Rueggeberg, Frederick A.
    Svizero, Nadia R.
    Pereira, Jose C.
    Pashley, David H.
    Carvalho, Ricardo M.
    JOURNAL OF ADHESIVE DENTISTRY, 2006, 8 (05): : 293 - 298
  • [32] MICROLEAKAGE OF COMPOSITE RESIN RESTORATIONS
    VONFRAUNHOFER, JA
    HAMMER, DW
    JOURNAL OF PROSTHETIC DENTISTRY, 1984, 51 (02): : 209 - 213
  • [33] Longevity of resin composite restorations
    Kubo, Shisei
    JAPANESE DENTAL SCIENCE REVIEW, 2011, 47 (01) : 43 - 55
  • [34] POROSITY IN COMPOSITE RESIN RESTORATIONS
    REINHARDT, JW
    JORDAN, RD
    DENEHY, GE
    RITTMAN, BRJ
    OPERATIVE DENTISTRY, 1982, 7 (03) : 82 - 85
  • [35] Bond strength of resin-resin interfaces contaminated with saliva and submitted to different surface treatments
    Furuse, Adilson Yoshio
    da Cunha, Leonardo Fernandes
    Benetti, Ana Raquel
    Mondelli, Jose
    JOURNAL OF APPLIED ORAL SCIENCE, 2007, 15 (06) : 501 - 505
  • [36] Microleakage of composite resin restorations
    Ballal, N. Vasudev
    AUSTRALIAN DENTAL JOURNAL, 2008, 53 (04)
  • [37] Resin-resin microtensile bond strength after different surface treatments to clean blood contamination
    Oliveira Carneiro, Dieiferson Thiers
    Generoso, Graziela Mendes
    Ferreira, Isana Aluares
    Dutra Borges, Boniek Castillo
    Rego de Freitas, Clebio Jarlison
    Araujo Santos Silva, Liliam Agna
    REVISTA PORTUGUESA DE ESTOMATOLOGIA MEDICINA DENTARIA E CIRURGIA MAXILOFACIAL, 2015, 56 (04): : 215 - 220
  • [38] Cross-sectional radiographic survey of amalgam and resin-based composite posterior restorations
    Levin, Liran
    Coval, Marius
    Geiger, Selly B.
    QUINTESSENCE INTERNATIONAL, 2007, 38 (06): : 511 - 514
  • [39] Effect of gingival fluid on marginal adaptation of Class II resin-based composite restorations
    Spahr, A
    Schön, F
    Haller, B
    AMERICAN JOURNAL OF DENTISTRY, 2000, 13 (05): : 261 - 266
  • [40] Dental cavity liners for Class I and Class II resin-based composite restorations
    Schenkel, Andrew B.
    Veitz-Keenan, Analia
    COCHRANE DATABASE OF SYSTEMATIC REVIEWS, 2019, (03):