The Influence of Multipass Friction Stir Processing on Formation of Microstructure and Mechanical Properties of Ti6Al4V Alloy

被引:9
作者
Zykova, A. P. [1 ]
Vorontsov, A. V. [1 ]
Chumaevskii, A., V [1 ]
Gurianov, D. A. [1 ]
Gusarova, A., V [1 ]
Savchenko, N. L. [1 ]
Kolubaev, E. A. [1 ]
机构
[1] Russian Acad Sci, Inst Strength Phys & Mat Sci, Siberian Branch, Tomsk 634055, Russia
关键词
friction stir processing; titanium alloys; phase transformations; grain size; wear resistance; ultimate strength; JOINT;
D O I
10.3103/S1067821222020146
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Friction stir processing (FSP) is an advanced technology of surface modification of microstructure of metals and alloys in order to improve mechanical and operational properties. Previous works on processing of titanium alloys demonstrated that variation of FSP process variables (such anticlockwise rotation rate, processing speed and plunge force) significantly influences on evolution of microstructure and mechanical properties of Ti6Al4V alloy. However, the influence of multipass FSP on Ti6Al4V alloy has not been studied. Thus, this work studied the influence of four-pass FSP of Ti6Al4V titanium alloy on evolution of microstructure and mechanical properties of this alloy. Analysis of the microstructure has demonstrated that, in the stir zone, a heterogeneous microstructure is formed with dynamically recrystallized equiaxial alpha and beta grains and beta regions with alpha phase of acicular and laminar types, which is related to the temperature gradient of the stir zone during FSP. It has been established that, with increase in the number of FSP passes to three, there is an increase in ultimate strength (up to 1173 MPa) and wear resistance (by 33%). Improvement of the ultimate strength after three passes of FSP is dictated by a decrease in grain size in the stir zone by 88% in comparison with the initial Ti6Al4V alloy. It has been demonstrated that, after four passes of FSP in the stir zone, an increase in the gain size and a decrease in the ultimate strength to 686 MPa occur, which is related to formation of coarse defects along the contours of metal flows. At the same time, the wear resistance of Ti6Al4V alloy after four passes of FSP increases by 39% in comparison with the initial material.
引用
收藏
页码:167 / 176
页数:10
相关论文
共 26 条
[1]  
Boyer R., 1994, TITANIUM ALLOYS MAT
[2]   Micro and macro mechanical characterization of friction stir welded Ti-6Al-4V lap joints through experiments and numerical simulation [J].
Buffa, Gianluca ;
Fratini, Livan ;
Schneider, Matthias ;
Merklein, Marion .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2013, 213 (12) :2312-2322
[3]   Modeling wear of cast Ti alloys [J].
Chan, Kwai S. ;
Koike, Marie ;
Okabe, Toru .
ACTA BIOMATERIALIA, 2007, 3 (03) :383-389
[4]  
Dong H., 2010, WOODHEAD PUBLISHING, DOI [10.1533/9781845699451, DOI 10.1533/9781845699451]
[5]   Surface Residual Stresses in Ti-6Al-4V Friction Stir Welds: Pre- and Post-Thermal Stress Relief [J].
Edwards, P. ;
Ramulu, M. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (09) :3263-3270
[6]   In situ observations of lattice expansion and transformation rates of α and β phases in Ti-6Al-4V [J].
Elmer, JW ;
Palmer, TA ;
Babu, SS ;
Specht, ED .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 391 (1-2) :104-113
[7]   Local mechanical properties, microstructure, and microtexture in friction stir welded Ti-6Al-4V alloy [J].
Fall, A. ;
Monajati, H. ;
Khodabandeh, A. ;
Fesharaki, M. H. ;
Champliaud, H. ;
Jahazi, M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 749 :166-175
[8]   Tool Wear Characteristics and Effect on Microstructure in Ti-6Al-4V Friction Stir Welded Joints [J].
Fall, Ameth ;
Fesharaki, Mostafa Hashemi ;
Khodabandeh, Ali Reza ;
Jahazi, Mohammad .
METALS, 2016, 6 (11)
[9]   Effect of microstructure, texture and deformation behavior on tensile properties of electrically assisted friction stir welded Ti-6Al-4 V joints [J].
Han, Yang ;
Chen, Shujun ;
Jiang, Xiaoqing ;
Bai, Yafeng ;
Yuan, Tao ;
Wang, Xuping .
MATERIALS CHARACTERIZATION, 2021, 176
[10]   Eliminating the tearing defect in Ti-6Al-4V alloy joint by back heating assisted friction stir welding [J].
Ji, Shude ;
Li, Zhengwei ;
Zhang, Liguo ;
Wang, Yue .
MATERIALS LETTERS, 2017, 188 :21-24