共 10 条
- [1] Corrosion behavior of alloy 316L stainless steel after exposure to supercritical water at 500 °C for 20,000 h JOURNAL OF SUPERCRITICAL FLUIDS, 2017, 127 : 191 - 199
- [3] Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water JOURNAL OF SUPERCRITICAL FLUIDS, 2007, 42 (01): : 157 - 163
- [4] Internal oxidation and crack susceptibility of alloy 310S stainless steel after long term exposure to supercritical water at 500 °C JOURNAL OF SUPERCRITICAL FLUIDS, 2017, 120 : 161 - 172
- [6] Corrosion and microstructural analysis data for AISI 316L and AISI 347H stainless steels after exposure to a supercritical water environment DATA IN BRIEF, 2016, 7 : 1341 - 1348
- [9] Carburization and Stress Profiles Characterized by High-Energy X-ray Diffraction in 316L Austenitic Stainless Steel After Exposure at 500 °C and 600 °C in Carburizing Liquid Sodium Oxidation of Metals, 2021, 96 : 185 - 199
- [10] Carburization and Stress Profiles Characterized by High-Energy X-ray Diffraction in 316L Austenitic Stainless Steel After Exposure at 500 °C and 600 °C in Carburizing Liquid Sodium OXIDATION OF METALS, 2021, 96 (3-4): : 185 - 199