Thermal and photochemical degradation of PPO/HIPS blends

被引:14
|
作者
Saron, Clodoaldo [1 ]
Sanchez, Elisabete M. S. [1 ]
Felisberti, Maria Isabel [1 ]
机构
[1] Univ Estadual Campinas, Inst Quim, BR-13083970 Campinas, SP, Brazil
关键词
blends; photochemical degradation; thermal degradation; mechanical properties;
D O I
10.1002/app.25671
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In general, polymer blends show a degradation behavior different from a simple combination of the individual components, making any forecast difficult without experiments. Interactions between polymers can sensibilize or stabilize the blend against degradation. In this work, the thermal and photooxidative degradation of blends of poly(2,6-dimethyl-1-1,4-phenylene oxide) (PPO) and high impact polystyrene (HIPS) have been studied under accelerated conditions. The extent of degradation was accompanied by infrared spectroscopy (FTIR) and Raman spectroscopy (FT-Raman) and impact resistance and strain-stress testing followed its influence on the macroscopic properties of the blends. The results showed that HIPS and the blend containing 60 wt% of PPO are more susceptible to thermal and photochemical degradation, while the blends containing 40 and 50 wt% of PPO are more stable. Infrared and Raman spectroscopic analyses showed that the degradation of HIPS and its blends is caused not only by degradation of the polybutadiene phase. Effects of interactions, such as exchange of energy in excited state between the PPO and PS components of the polymeric matrix may also be responsible for the degradation and loss of mechanical properties of the PPO/HIPS blends. The chemical degradation directly affects the mechanical properties of the samples with photodegradation being more harmful than the thermal degradation at 75 degrees C. (c) 2007 Wiley Periodicals, Inc.
引用
收藏
页码:3269 / 3276
页数:8
相关论文
共 50 条
  • [31] Thermal degradation of blends of PVC with polysiloxane - 1
    Zulfiqar, S
    Ahmad, S
    POLYMER DEGRADATION AND STABILITY, 1999, 65 (02) : 243 - 247
  • [32] Thermal degradation of blends of PVAC with polysiloxane - II
    Zulfiqar, S
    Ahmad, S
    POLYMER DEGRADATION AND STABILITY, 2001, 71 (02) : 299 - 304
  • [33] Thermal degradation of polystyrene-polydimethylsiloxane blends
    Lomakin, SM
    Koverzanova, EV
    Shilkina, NG
    Usachev, SV
    Zaikov, GE
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2003, 76 (03) : 472 - 482
  • [34] Thermal Degradation of Polystyrene-Polydimethylsiloxane Blends
    1600, Maik Nauka-Interperiodica Publishing (76):
  • [35] Thermal Degradation of Polystyrene-Polydimethylsiloxane Blends
    S. M. Lomakin
    E. V. Koverzanova
    N. G. Shilkina
    S. V. Usachev
    G. E. Zaikov
    Russian Journal of Applied Chemistry, 2003, 76 : 472 - 482
  • [36] COMPATIBILITY AND TENSILE PROPERTIES OF PPO BLENDS
    FRIED, JR
    KARASZ, FE
    MACKNIGHT, WJ
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1979, (APR): : 202 - 202
  • [37] THERMAL AND THERMAL OXIDATIVE-DEGRADATION OF POLYCYANURATES AND THEIR BLENDS WITH POLYGLYCIDETHERS
    BAUER, M
    GNAUCK, R
    ACTA POLYMERICA, 1987, 38 (12) : 658 - 661
  • [38] Degradation and aging of polymer blends -: I.: Thermomechanical and thermal degradation
    Pospísil, J
    Horák, Z
    Krulis, Z
    Nespurek, S
    Kuroda, S
    POLYMER DEGRADATION AND STABILITY, 1999, 65 (03) : 405 - 414
  • [39] THERMAL AND PHOTOCHEMICAL STABILITY OF POLYSTYRENE AND ITS BLENDS WITH POLYVINYL-CHLORIDE .2. PHOTOCHEMICAL TRANSFORMATION IN POLYSTYRENE BLENDS WITH POLYVINYL-CHLORIDE, AND THEIR THERMAL-STABILITY
    KAMINSKA, A
    SANYAL, S
    KACZMAREK, H
    JOURNAL OF THERMAL ANALYSIS, 1989, 35 (07): : 2135 - 2141
  • [40] Thermal and photochemical degradation of dimethylsulfoxide on TiO2
    Huang, Sin-Jhang
    Lin, Yu-Cheng
    Lin, Jong-Liang
    CHEMICAL PHYSICS LETTERS, 2012, 549 : 17 - 21