Electrical arc phenomena and its interaction on contact material at 42 volts DC for automotive applications

被引:26
作者
Doublet, L [1 ]
Ben Jemaa, N [1 ]
Hauner, F [1 ]
Jeannot, D [1 ]
机构
[1] Univ Rennes 1, PALMS Lab, F-35042 Rennes, France
来源
ELECTRICAL CONTACTS-2004: PROCEEDINGS OF THE 50TH IEEE HOLM CONFERENCE ON ELECTRICAL CONTACTS/THE 22ND INTERNATIONAL CONFERENCE ON ELECTRICAL CONTACTS | 2004年
关键词
D O I
10.1109/HOLM.2004.1353087
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
In order to fulfill the increasing needs of electrical power in automobiles, the electrical network, currently at 14 VDC, must be changed to 42 VDC. This involves that switching DC devices will have to be improved to insure reliability and electrical safety. Therewith, for improve comprehension of arc phenomena and its interactions with contact materials under 42 VDC, the authors undertook a study on this subject. This paper summarizes the whole of work and tackles the arc phenomena at break and make, the contact material transfer and the problems of welding at make. Thus, we studied break arc duration, arc length (gap) and material transfer versus the effect of material, opening speed and loads. We have established that the arc duration and its length are extremely extended by a few millimeters compared to the arc in 14 VDC. At 42 VDC and low current, erosion and transfer direction is similar to the previous one obtained at low arcing length in 14 VDC. But at large gap, with 42 VDC inductive loads or high current, new mechanism erosion mode takes place which induce the cathode and the anode loss. Erosion and arc length of AgSnO2 contacts is higher than other material: for this particular behavior, some complementary investigations, using X chemical analysis, have been undertaken. It seems that electrical arc enriches in tin element the contacts surfaces leading to this behavior. In other way, we have investigated make arc erosion, welding tendency and welding forces for all materials. It was found that contrary to the 14 VDC case, the make are takes place during the total bounce period. The rating material performances at make seem to be reversed than at break. This study enables to understand the material effect at this higher voltage and thus should allow the improvement of the material itself, Anyway, the commutation devices of 42 VDC should employ improved materials and also additional systems of arc reduction.
引用
收藏
页码:8 / 14
页数:7
相关论文
共 10 条
[1]  
BELHACHEMI B, 1984, 12 ICEC HOLM C CHIC, P475
[2]  
Ben Jemaa N, 2002, ELECTRICAL CONTACTS-2002: PROCEEDINGS OF THE FORTY-EIGHTH IEEE HOLM CONFERENCE ON ELECTRICAL CONTACTS, P128, DOI 10.1109/HOLM.2002.1040832
[3]   Break arc study for the new electrical level of 42 V in automotive applications [J].
Ben Jemaa, N ;
Doublet, L ;
Morin, L ;
Jeannot, D .
PROCEEDINGS OF THE FORTY-SEVENTH IEEE HOLM CONFERENCE ON ELECTRICAL CONTACTS, 2001, :50-55
[4]   Anodic and cathodic erosion of Ag, Ag alloys and Ag-MeO contact materials in energy range below 10 joules [J].
BenJemaa, N ;
Nedelec, L ;
Benhenda, S ;
Neveu, J .
ELECTRICAL CONTACTS - 1996: PROCEEDINGS OF THE FORTY-SECOND IEEE HOLM CONFERENCE ON ELECTRICAL CONTACTS: JOINT WITH THE 18TH INTERNATIONAL CONFERENCE ON ELECTRICAL CONTACTS, 1996, :70-74
[5]  
BENJEMAA N, 2002, P 48 IEEE HOLM C EC
[6]   Make arc erosion and welding tendency under 42 VDC in automotive area [J].
Doublet, L ;
Ben Jemaa, N ;
Hauner, F ;
Jeannot, D .
PROCEEDINGS OF THE FORTY-NINTH IEEE HOLM CONFERENCE ON ELECTRICAL CONTACTS, 2003, :158-162
[7]  
HETZMANNSEDER E, 1994, IEEE T CPMT A, V17, P61
[8]   Transition from the anodic arc phase to the cathodic metallic arc phase in vacuum at low DC electrical level [J].
Morin, L ;
Ben Jemaa, N ;
Jeannot, D ;
Sone, H .
PROCEEDINGS OF THE FORTY-SEVENTH IEEE HOLM CONFERENCE ON ELECTRICAL CONTACTS, 2001, :88-93
[9]   Make arc erosion and welding in the automotive area [J].
Morin, L ;
Ben Jemaa, N ;
Jeannot, D .
IEEE TRANSACTIONS ON COMPONENTS AND PACKAGING TECHNOLOGIES, 2000, 23 (02) :240-246
[10]  
NEDELEC L, 1997, THESIS U RENNES1 FRA