Oxidation behavior of C-SiC composites with a Si-W coating from room temperature to 1500°C

被引:17
|
作者
Cheng, LF [1 ]
Xu, YD [1 ]
Zhang, LT [1 ]
Gao, R [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
关键词
carbon-carbon composites; coating; oxidation;
D O I
10.1016/S0008-6223(00)00066-X
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Oxidation tests of carbon fiber reinforced silicon carbide composites with a Si-W coating were conducted in dry air from room temperature to 1500 degreesC for 5 h. A continuous series of empirical functions relating weight change to temperature after 5 h oxidation was found to fit the test results quite well over the whole temperature range. This approach was used to interpret the different oxidation mechanisms. There were two cracking temperatures of the matrix and the coating for the C-SIC composite. Oxidation behavior of the C-SIC composite was nearly the same as that of the coated C-C composite above the coatings cracking temperature, but weight loss of the C-SiC composite was half an order lower than that of the coated C-C composite below the cracking temperature. As an inhibitor, the SiC matrix increased the oxidation resistance of C-SiC composites by decreasing active sites available for oxidation. As an interfacial layer, pyrolytic carbon decreased the activation energy below 700 degreesC. From 800 degreesC to 1030 degreesC, uniform oxidation took place for the C-SiC composite, but non-uniform oxidation took place for the coated C-C composite in the same temperature range. The Knudsen diffusion coefficient could be used to explain the relationship between weight loss and temperature below the coating cracking temperature and the matrix cracking temperature. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2133 / 2138
页数:6
相关论文
共 50 条
  • [31] Bonding strength, thermal shock and oxidation resistance of interlocking (Zr,Hf)C-SiC/SiC double-layer coating for C/C composites
    Zhuang, Lei
    Fu, Qian-Gang
    SURFACE & COATINGS TECHNOLOGY, 2017, 315 : 436 - 442
  • [32] Oxidation behavior of SiC-HfB2-Si coating on C/C composites prepared by slurry dipping combined with gaseous Si infiltration
    Zhang, Pei
    Fu, Qian-gang
    Hu, Dou
    Cheng, Chun-yu
    Zhu, Xiao-fei
    SURFACE & COATINGS TECHNOLOGY, 2020, 385
  • [33] HfC nanowires to improve the toughness and oxidation resistance of Si-Mo-Cr/SiC coating for C/C composites
    Ren, Jincui
    Zhang, Yulei
    Hu, Heng
    Zhang, Pengfei
    Fei, Tian
    Zhang, Leilei
    CERAMICS INTERNATIONAL, 2016, 42 (13) : 14518 - 14525
  • [34] Effect of Mo/Si Ratio on the Microstructure and Oxidation Resistance of Si-Mo Coating for C/C Composites
    Zhang Yulei
    Li Hejun
    Fu Qiangang
    Li Kezhi
    Ouyang Haibo
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 : 109 - 112
  • [36] Oxidation behavior of carbon-carbon composites with a three-layer coating from room temperature to 1700°C
    Cheng, LF
    Xu, YD
    Zhang, LT
    Yin, XW
    CARBON, 1999, 37 (06) : 977 - 981
  • [37] W-Mo-Si/SiC oxidation protective coating for carbon/carbon composites
    Hou, Dangshe
    Li, Kezhi
    Li, Hejun
    Fu, Qiangang
    Wei, Jian
    Zhang, Yulei
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2007, 23 (04) : 559 - 562
  • [38] Oxidation failure behavior and repair of the damaged SiC-ZrB2/SiC 2 /SiC coating of C/C composites
    Wang, Weiyan
    Hu, Jingbo
    Tang, Yufei
    Fu, Qiangang
    APPLIED SURFACE SCIENCE, 2024, 673
  • [39] Microstructural evolution of SiC coating on C/C composites exposed to 1500 °C in ambient air
    Zhou, Wei
    Xiao, Peng
    Luo, Wei
    Li, Yang
    CERAMICS INTERNATIONAL, 2019, 45 (01) : 854 - 860
  • [40] Structure and oxidation behaviors of C/C-SiC coated with Al2O3-CrAl0.42Si1.58-SiC-Al4SiC4 oxidation protection system
    Jiao Geng-Sheng
    Li He-Jun
    Lu Guo-Feng
    ADVANCED COMPOSITE MATERIALS, 2012, 21 (04) : 273 - 281