Kinetics of high temperature corrosion of a low Cr-Mo steel in aqueous NaCl Solution

被引:1
作者
Bayoumi, F. M. [1 ]
机构
[1] Cent Met Res & Dev Inst, Dept Surface Modificat & Protect, Cairo, Egypt
来源
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION | 2007年 / 58卷 / 06期
关键词
D O I
10.1002/maco.200604028
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The kinetics of corrosion of a low Cr-Mo steel alloy were studied over the temperature range of 75-250 degrees C in 1 m NaCl in absence and in presence of various levels of contamination with CuCl2. Corrosion rates, weights of corrosion product (magnetite) film and total (integral) weight loss of the alloy over exposure times from I up to 480 h were measured. The corrosion rate decreases rapidly with time, before it levels off at longer time, indicating the formation of a protective corrosion product film. The ability of the alloy to retain an adherent corrosion product (magnetite) film was expressed in terms of a retention coefficient. This was found to increase with temperature and exposure time and to decrease with the level of contamination with CuCl2. This effect of temperature was attributed to the improvement of the crystallinity of the corrosion product. On the other hand, the effect of CuCl2 was attributed to the electrodeposition of Cu and its impregnation within the corrosion product, which becomes less adherent. The free corrosion potential was found to be affected by the presence of the CuCl2, in a fashion compatible with the Wagner-Traud theory of mixed potential.
引用
收藏
页码:422 / 426
页数:5
相关论文
共 50 条
  • [11] Ageing effects on α' precipitation and resistance to corrosion of a novel Cr-Mo stainless steel with high Mo content
    Vasconcelos, Igor F.
    Tavares, Sergio S. M.
    Reis, F. Evaristo U.
    Abreu, Hamilton F. G.
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (01) : 293 - 299
  • [12] IMPROVEMENT OF LOW-TEMPERATURE NOTCH TOUGHNESS IN Cr-Mo STEEL WELDS.
    Yamamoto, Shigeaki
    Natsume, Syogo
    R and D: Research and Development Kobe Steel Engineering Reports, 1985, 35 (03): : 44 - 47
  • [13] EFFECTS OF HOLDING TEMPERATURE ON BAINITE TRANSFORMATION IN CR-MO STEEL
    Sarizam, M.
    Komizo, Y.
    JOURNAL OF MECHANICAL ENGINEERING AND SCIENCES, 2014, 7 : 1103 - 1114
  • [14] Deformation Characteristics and Dynamic Recrystallization Model of Cr-Mo High Temperature Ferritic Steel
    Luo R.
    Chen L.
    Cao Y.
    Zhou H.
    Cui S.
    Han M.
    Pei C.
    Cheng X.
    Gao P.
    Cailiao Daobao/Materials Reports, 2020, 34 (20): : 20118 - 20122
  • [15] Solute grain boundary segregation during high temperature plastic deformation in a Cr-Mo low alloy steel
    Chen, X. -M.
    Song, S. -H.
    Weng, L. -Q.
    Liu, S. -J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (25-26): : 7663 - 7668
  • [16] COERCIVITY AND MICROSTRUCTURE OF LOW-ALLOY CR-MO STEEL
    STERNBERK, J
    KRATOCHVILOVA, E
    HREBIK, J
    GEMPERLE, A
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1983, 79 (02): : 523 - 529
  • [17] Toughness degradation of two sets of Cr-Mo steel high temperature turbine bolts
    Bulloch, JH
    ECF 11 - MECHANISMS AND MECHANICS OF DAMAGE AND FAILURE, VOLS I-III, 1996, : 2019 - 2023
  • [18] CREEP FRACTURE OF CR-MO STEEL
    RADHAKRISHNAN, VM
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1992, 15 (06) : 617 - 623
  • [19] EMBRITTLEMENT OF A Cr-Mo LOW-ALLOY STEEL DUE TO LOW-TEMPERATURE NEUTRON IRRADIATION
    S.H. Song and L.Q. Weng Department of Materials Science and Engineering
    ActaMetallurgicaSinica(EnglishLetters), 2006, (01) : 20 - 26
  • [20] Embrittlement of a Cr-Mo low-alloy steel due to low-temperature neutron irradiation
    Song, S.H.
    Weng, L.Q.
    Acta Metallurgica Sinica (English Letters), 2006, 19 (01) : 20 - 26