The effect of electrode potential on stress corrosion cracking in highly sensitized Al-Mg alloys

被引:32
作者
McMahon, M. E. [1 ]
Harris, Z. D. [1 ]
Scully, J. R. [1 ]
Burns, J. T. [1 ]
机构
[1] Univ Virginia, Ctr Electrochem Sci & Engn, Dept Mat Sci & Engn, Charlottesville, VA 22904 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2019年 / 767卷
关键词
ENVIRONMENTALLY ASSISTED CRACKING; RICH EPOXY PRIMER; INTERGRANULAR CORROSION; HYDROGEN EMBRITTLEMENT; CATHODIC POLARIZATION; ALUMINUM-ALLOYS; ELECTROCHEMICAL-BEHAVIOR; MECHANICAL-PROPERTIES; PURITY ALUMINUM; STAINLESS-STEEL;
D O I
10.1016/j.msea.2019.138399
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The potential dependence of intergranular environmental cracking phenomena in highly sensitized AA5456-H116 is defined in Cl--containing solution. Stress corrosion cracking (SCC) occurrence is compared with the propensity for corrosion attack, subsequent alloy degradation, and gaseous H evolution/H absorption phenomena as a function of potential in both the anodic and cathodic polarization regions. The SCC susceptibility is low (threshold stress intensity for SCC (K-TH) approaching the fracture toughness) in Al-Mg under cathodic polarization conditions and high when anodically polarized (low K-TH). The lack of environmental cracking susceptibility was directly proportional to low area normalized levels of H generation estimated to occur at the crack tip at each polarization level. Chemical blunting is shown to be an operative phenomenon at the crack tip to suppress cathodic crack growth by attenuating the mechanical driving force. This blunting phenomenon is demonstrated to have no effect on the threshold stress intensity or crack growth rate for SCC during anodic crack growth where the crack tip readily re-sharpens through the IGC/beta phase dissolution process followed by H-induced crack advance.
引用
收藏
页数:19
相关论文
共 147 条
  • [1] Influence of the cathodic intermetallics distribution on the reproducibility of the electrochemical measurements on AA5083 alloy in NaCl solutions
    Aballe, A
    Bethencourt, M
    Botana, FJ
    Cano, M
    Marcos, M
    [J]. CORROSION SCIENCE, 2003, 45 (01) : 161 - 180
  • [2] Localized alkaline corrosion of alloy AA5083 in neutral 3.5% NaCl solution
    Aballe, A
    Bethencourt, M
    Botana, FJ
    Cano, MJ
    Marcos, M
    [J]. CORROSION SCIENCE, 2001, 43 (09) : 1657 - 1674
  • [3] Effective Hydrogen Diffusion in Aluminum Alloy 5083-H131 as a Function of Orientation and Degree of Sensitization
    Ai, Jia-He
    Lim, Mary Lyn C.
    Scully, John R.
    [J]. CORROSION, 2013, 69 (12) : 1225 - 1239
  • [4] Hydrogen Diffusivity During Corrosion of High-Purity Aluminum
    Ai, Jia-He
    Scully, John R.
    [J]. CORROSION, 2013, 69 (08) : 752 - 767
  • [5] Electrochemical hydrogen permeation tests under galvanostatic hydrogen charging conditions conventionally used for hydrogen embrittlement study
    Akiyama, Eiji
    Li, Songjie
    [J]. CORROSION REVIEWS, 2016, 34 (1-2) : 103 - 112
  • [6] [Anonymous], 2009, ASTM STAND, DOI [10.1520/E1447-09R16.2, DOI 10.1520/E1447-09R16.2]
  • [7] [Anonymous], 2004, G6704 ASTM INT
  • [8] [Anonymous], 1998, Corros. NACE
  • [9] [Anonymous], 2010, CRC HDB CHEM PHYS
  • [10] [Anonymous], 2004, ANN BOOK ASTM STAND, DOI [10.1520/G0067-04.2., DOI 10.1520/G0067-04.2]