A degradation study of PLLA containing lauric acid

被引:30
作者
Renouf-Glauser, AC
Rose, J
Farrar, D
Cameron, RE
机构
[1] Univ Cambridge, Dept Mat Sci & Met, Cambridge CB2 3QZ, England
[2] Smith & Nephew Grp Res Ctr, York YO10 5DF, N Yorkshire, England
基金
英国工程与自然科学研究理事会;
关键词
polylactic acid; degradation; mechanical properties; x-ray diffraction (XRD); microstructure;
D O I
10.1016/j.biomaterials.2004.07.067
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Addition of lauric acid to Poly (L-lactide) (PLLA) has resulted in a new family of enhanced degradation biomaterials. Presented is PLLA4.5 (PLLA containing 4.5 wt% lauric acid), the fastest degrading of the family. Degradation was studied via mass changes, gel-permeation chromatography, wide- and small-angle X-ray scattering (WAXS and SAXS), simultaneous SAXS and tensile testing, and visual observation. The undegraded PLLA4.5 deformed by crazing, recognisable from the characteristic shape of the SAXS pattern. As water up-take and degradation proceeded,samples crystallised, decreasing the SAXS long period, until by 4 days the deformation mechanism had become that of crystal-mediated deformation. This resulted in a 'peanut lemon'-shaped SAXS pattern, interpreted in terms of cavitation and fibrillated shear. Further degradation up to 12 days resulted in the same deformation mechanism at different sample displacements, with samples failing earlier during tensile testing until a ductile-brittle transition occurred. At 30-40 days water up-take and mass-loss increased significantly and global whitening of samples occurred, while the crystallinity and long period stabilised. Complete degradation had not occurred by the end of the study at 73 days. Through an understanding of how the changes in morphology during degradation affect the micromechanisms of deformation, it may be possible to design microstructures to give a tailored evolution of mechanical response in the body. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2415 / 2422
页数:8
相关论文
共 34 条
[1]  
[Anonymous], 1991, INTRO POLYM
[2]   CRAZE MICROSTRUCTURE FROM SMALL-ANGLE X-RAY-SCATTERING (SAXS) [J].
BROWN, HR ;
KRAMER, EJ .
JOURNAL OF MACROMOLECULAR SCIENCE-PHYSICS, 1981, B19 (03) :487-522
[3]   A real-time simultaneous small- and wide-angle X-ray scattering study of in situ polyethylene deformation at elevated temperatures [J].
Butler, MF ;
Donald, AM .
MACROMOLECULES, 1998, 31 (18) :6234-6249
[4]   THE BIODEGRADABILITY OF POLYESTER BLENDS [J].
CHA, Y ;
PITT, CG .
BIOMATERIALS, 1990, 11 (02) :108-112
[5]  
Elias H., 1997, INTRO POLYM SCI
[6]   INVESTIGATION OF STRUCTURE OF SOLUTION GROWN CRYSTALS OF LACTIDE COPOLYMERS BY MEANS OF CHEMICAL-REACTIONS [J].
FISCHER, EW ;
STERZEL, HJ ;
WEGNER, G .
KOLLOID-ZEITSCHRIFT AND ZEITSCHRIFT FUR POLYMERE, 1973, 251 (11) :980-990
[7]   HYDROLYTIC DEGRADATION OF DEVICES BASED ON POLY(DL-LACTIC ACID) SIZE-DEPENDENCE [J].
GRIZZI, I ;
GARREAU, H ;
LI, S ;
VERT, M .
BIOMATERIALS, 1995, 16 (04) :305-311
[8]   GENERAL CRYSTALLIZATION BEHAVIOR OF POLY(L-LACTIC ACID) [J].
KALB, B ;
PENNINGS, AJ .
POLYMER, 1980, 21 (06) :607-612
[9]  
KULKARNI R K, 1971, Journal of Biomedical Materials Research, V5, P169, DOI 10.1002/jbm.820050305
[10]   RESORBABLE MATERIALS OF POLY(L-LACTIDE) .6. PLATES AND SCREWS FOR INTERNAL FRACTURE FIXATION [J].
LEENSLAG, JW ;
PENNINGS, AJ ;
BOS, RRM ;
ROZEMA, FR ;
BOERING, G .
BIOMATERIALS, 1987, 8 (01) :70-73