Hydrothermal synthesis and properties of Ce1-xSmxO2-x/2 and Ce1-xCaxO2-x solid solutions

被引:145
|
作者
Huang, W [1 ]
Shuk, P [1 ]
Greenblatt, M [1 ]
机构
[1] RUTGERS STATE UNIV,DEPT CHEM,PISCATAWAY,NJ 08855
关键词
D O I
10.1021/cm970425t
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The structure, thermal expansion coefficients and ionic conductivity of Ce1-xSmxO2-x/2 and Ce1-xCaxO2-x (x = 0-0.30) solid electrolytes prepared hydrothermally in a relatively wide concentration range for the first time were systematically investigated. The uniformly small particle size (40-68 nm) of the hydrothermally prepared materials allows sintering of the samples into highly dense ceramic pellets at 1400 degrees C, a significantly lower temperature, compared to that at 1600 degrees C required for samples prepared by solid-state techniques. The maximum ionic conductivity was found at x = 0.17 for the Sm and at x = 0.09 for the Ca-substituted ceria (sigma(600 degrees C) = 5.7 x 10(-3) S/cm, E-a approximate to 0.9 eV, and sigma(600 degrees C) = 2.1 x 10(-3) S/cm, E-a approximate to 0.8 eV, respectively). The thermal expansion coefficients, determined from high-temperature X-ray data, are 8.6 x 10(-6) and 9.4 x 10(-6) K-1 for the best conducting Ce0.83Sm0.17O1.915 and Ce0.91Ca0.09O1.91 solid electrolytes, respectively.
引用
收藏
页码:2240 / 2245
页数:6
相关论文
共 50 条
  • [31] Hydrothermal synthesis and properties of mixed conductors based on Ce1-xPrxO2-δ solid solutions
    Shuk, P
    Greenblatt, M
    SOLID STATE IONICS, 1999, 116 (3-4) : 217 - 223
  • [32] Hydrothermal synthesis and properties of mixed conductors based on Ce1-xPrxO2-δ solid solutions
    State Univ of New Jersey, Piscataway, United States
    Solid State Ionics, 3-4 (217-223):
  • [33] Electroconduction and linear expansion of solid electrolytes Ce1−xSmxO2−δ (x = 0.10−0.30)
    E. G. Vaganov
    V. P. Gorelov
    N. M. Bogdanovich
    I. V. Korzun
    V. A. Kazantsev
    Russian Journal of Electrochemistry, 2007, 43 : 663 - 666
  • [34] Synthesis of One-Dimensional Ce1-xYxO2-x/2 (0 ≤ x ≤ 1) Solid Solutions and Their Catalytic Properties: The Role of Oxygen Vacancies
    Yang, Dan
    Wang, Lei
    Sun, Yangzhao
    Zhou, Kebin
    JOURNAL OF PHYSICAL CHEMISTRY C, 2010, 114 (19): : 8926 - 8932
  • [35] Electroconduction and linear expansion of solid electrolytes Ce1-xSmxO2-δ(x 0.10-0.30)
    Vaganov, E. G.
    Gorelov, V. P.
    Bogdanovich, N. M.
    Korzun, I. V.
    Kazantsev, V. A.
    RUSSIAN JOURNAL OF ELECTROCHEMISTRY, 2007, 43 (06) : 663 - 666
  • [36] Hydrothermal synthesis and characterization of nanometer Ce1-xCoxO2-δ solid solutions
    Zhang Guo-Fang
    Xue Yan-Feng
    Xu Jiao-Xing
    Qiu Xiao-Qing
    Li Guang-She
    Li Li-Ping
    CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 2007, 28 (04): : 603 - 607
  • [37] Synthesis and Properties of the Solid Solution Ce1-xPrxO2-δ (x=0.05∼0.30)
    Lin Xiaomin
    Yan Shi
    Zhu Lili
    Li Liping
    Su Wenhui
    ACTA CHIMICA SINICA, 2009, 67 (12) : 1389 - 1394
  • [38] Microstructure and Electrical Properties of Ce1-xScxO2-x/2 Solid Electrolyte
    Xue Y.
    Peng J.
    Li S.
    An S.
    Zhongguo Xitu Xuebao/Journal of the Chinese Rare Earth Society, 2019, 37 (04): : 473 - 480
  • [39] Synthesis and characterization of nano-crystalline Ce1-xGdxO2-x/2 (x=0-0.30) solid solutions
    Jadhav, L. D.
    Chourashiya, M. G.
    Jamale, A. P.
    Chavan, A. U.
    Patil, S. P.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 506 (02) : 739 - 744
  • [40] Mechanosynthesis and Sintering of Ce1-xYxO2-δ (x ≤ 0.35) Solid Solutions
    Fabian, M.
    Briancin, J.
    Schutz, T.
    ACTA PHYSICA POLONICA A, 2014, 126 (04) : 951 - 953