Impact fretting wear of Inconel 690 tube with different supporting structure under cycling low kinetic energy

被引:32
作者
Sun, Yang [1 ]
Cai, Zhen-bing [1 ]
Chen, Zhi-qiang [1 ]
Qian, Hao [2 ]
Tang, Li-chen [2 ]
Xie, Yongcheng [2 ]
Zhou, Zhong-rong [1 ]
Zhu, Min-hao [1 ]
机构
[1] Southwest Jiaotong Univ, Tribol Res Inst, Key Lab Adv Technol Mat, Chengdu 610031, Peoples R China
[2] Shanghai Nucl Engn Res & Design Inst, Shanghai 200233, Peoples R China
基金
中国国家自然科学基金;
关键词
Impact fretting wear; Impact kinetic energy; Supporting structure; Inconel; 690; STEAM-GENERATOR TUBE; BEHAVIOR; ALLOY; WATER; TEMPERATURES;
D O I
10.1016/j.wear.2017.01.011
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The impact fretting wear behavior of a 690 alloy tube affected by low-impact cycling kinetic energy was investigated. The Inconel 690 alloy specimen was clamped by cantilever and simple supported beam structures for support. The interface response was affected by the clamping situation, and material wear was affected by the change in the interface response. The energy loss, contact force versus time and frequency, energy absorption, and deformation of the material (thin wall tube) during impact were analyzed. The worn surfaces and cross-sectional morphologies were observed with an optical microscope and a 2D surface profiler to analyze the impact fretting wear mechanism under the two support structures. In the two clamping structures, wear decreased when the span increased, and material wear showed a high correlation with the peak impact force and absorbed energy. The wear mechanism of the alloy 690 specimen was delamination. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:625 / 633
页数:9
相关论文
共 26 条
[1]  
[Anonymous], 2000, Impact mechanics
[2]  
[Anonymous], 1994, Dynamic Behavior of Materials, P66
[3]   New parameter for characterizing and correlating impact-sliding fretting wear to energy dissipation-experimental investigation [J].
Attia, Helmi ;
Gessesse, Y. B. ;
Osman, M. O. M. .
WEAR, 2007, 263 (1-6 SPEC. ISS.) :419-429
[4]   MATERIALS REQUIREMENTS FOR PRESSURIZED WATER-REACTOR STEAM-GENERATOR TUBING [J].
BERGE, P ;
DONATI, JR .
NUCLEAR TECHNOLOGY, 1981, 55 (01) :88-104
[5]   High temperature sliding wear behaviour of Inconel 617 and Stellite 6 alloys [J].
Birol, Yucel .
WEAR, 2010, 269 (9-10) :664-671
[6]   Impact fretting wear behavior of 304 stainless steel thin-walled tubes under low-velocity [J].
Cai, Zhen-Bing ;
Guan, Hai-Da ;
Chen, Zhi-Qiang ;
Qian, Hao ;
Tang, Li-Chen ;
Zhou, Zhong-Rong ;
Zhu, Min-Hao .
TRIBOLOGY INTERNATIONAL, 2017, 105 :219-228
[7]  
Cheng ZQ., 2016, J MECH ENG, V8, P79
[8]   Overview of steam generator tube degradation and integrity issues [J].
Diercks, DR ;
Shack, WJ ;
Muscara, J .
NUCLEAR ENGINEERING AND DESIGN, 1999, 194 (01) :19-30
[9]  
ENGEL PA, 1995, WEAR, V181, P730
[10]   Vibration thresholds for fretting corrosion in electrical connectors [J].
Flowers, GT ;
Xie, F ;
Bozack, MJ ;
Malucci, RD .
IEEE TRANSACTIONS ON COMPONENTS AND PACKAGING TECHNOLOGIES, 2004, 27 (01) :65-71