The use of alkaline CO2 solvent for the CO2 curing of blast-furnace slag mortar

被引:11
作者
Han, Seong Ho [1 ]
Jun, Yubin [1 ]
Kim, Jae Hong [1 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Civil & Environm Engn, 291 Daehak Ro, Daejeon 34141, South Korea
关键词
Alkali-activated slag; Direct aqueous carbonation; CCUS; CO2; curing; COMPRESSIVE STRENGTH; PORE SOLUTION; CEMENT; CARBONATION; HYDRATION; CONCRETE; MICROSTRUCTURE; WATER;
D O I
10.1016/j.conbuildmat.2022.127977
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Moving toward carbon neutrality in the construction industry involves utilizing CO2 to produce construction materials. CO2 curing of cement-based materials induces carbonation at an early age, which enhances strength and performance. A new process for the CO2 curing is proposed using CO2-dissolved curing water, which needs no massive CO2-gas chamber encasing cement-based materials in mild pressure. Gaseous CO2 was dissolved in 1 M aqueous KOH solution beforehand, and mortar samples made with ground-granulated blast furnace slag were submerged and cured. The CO2-water curing for 3 days carbonated the samples, but was not beneficial for their 3-day strengths. Successive moist curing resulted in further hydration of the mortar with carbonate seeds. Finally, the samples' strengths at 28 days were enhanced, and their CO2 uptake was as much as the conventional CO2 curing provides.
引用
收藏
页数:10
相关论文
共 42 条
[1]  
[Anonymous], 2009, ISO: 679
[2]  
[Anonymous], 2008, ASTM C109
[3]   Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags [J].
Ben Haha, M. ;
Le Saout, G. ;
Winnefeld, F. ;
Lothenbach, B. .
CEMENT AND CONCRETE RESEARCH, 2011, 41 (03) :301-310
[4]  
BERGER RL, 1972, NATURE-PHYS SCI, V240, P16, DOI 10.1038/physci240016a0
[5]   A STUDY ON THE REACTION BETWEEN CO2 AND ALKANOLAMINES IN AQUEOUS-SOLUTIONS [J].
BLAUWHOFF, PMM ;
VERSTEEG, GF ;
VANSWAAIJ, WPM .
CHEMICAL ENGINEERING SCIENCE, 1983, 38 (09) :1411-1429
[6]   Global CO2 Emission-Related Geotechnical Engineering Hazards and the Mission for Sustainable Geotechnical Engineering [J].
Chang, Ilhan ;
Lee, Minhyeong ;
Cho, Gye-Chun .
ENERGIES, 2019, 12 (13)
[7]   Solubility of CO2 in water from -1.5 to 100°C and from 0.1 to 100 MPa:: evaluation of literature data and thermodynamic modelling [J].
Diamond, LW ;
Akinfiev, NN .
FLUID PHASE EQUILIBRIA, 2003, 208 (1-2) :265-290
[8]   Alkali-activated slag mortars -: Mechanical strength behaviour [J].
Fernández-Jiménez, A ;
Palomo, JG ;
Puertas, F .
CEMENT AND CONCRETE RESEARCH, 1999, 29 (08) :1313-1321
[9]   STRUCTURE OF ALKALI METALS IN LIQUID STATE [J].
GINGRICH, NS ;
HEATON, L .
JOURNAL OF CHEMICAL PHYSICS, 1961, 34 (03) :873-&
[10]   CO2 Curing Efficiency for Cement Paste and Mortars Produced by a Low Water-to-Cement Ratio [J].
Han, Seong Ho ;
Jun, Yubin ;
Shin, Tae Yong ;
Kim, Jae Hong .
MATERIALS, 2020, 13 (17)