EFFECT OF WOOD FLOUR AND NANO-CaCO3 CONTENT ON THE PROPERTIES OF NANO-CaCO3/WOOD FLOUR/POLYPROPYLENE INJECTION MOLDED COMPOSITES

被引:0
作者
Ahmadi, Amirhossein [1 ]
Bazyar, Behzad [1 ]
Eslam, Habibollah Khademi [1 ]
Azizi, Hamed [2 ]
机构
[1] Islamic Azad Univ, Coll Agr & Nat Resources, Dept Wood & Paper Sci & Technol, Sci & Res Branch, Tehran, Iran
[2] IPPI, Dept Proc, POB 14965-115, Tehran, Iran
来源
CELLULOSE CHEMISTRY AND TECHNOLOGY | 2018年 / 52卷 / 5-6期
关键词
composites; wood flour; polypropylene; nano-calcium carbonate; injection molding; tensile strength; tensile modulus; hardness; MECHANICAL-PROPERTIES; POLYPROPYLENE COMPOSITES; POLYETHYLENE COMPOSITES; PLASTIC COMPOSITES; POLYMER COMPOSITES; WATER-ABSORPTION; CACO3; PARTICLES; NANOCLAY; SIZE; NANOCOMPOSITES;
D O I
暂无
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
This study evaluated the effect of wood flour and nano-CaCO3 contents on some properties of nano-CaCO3/wood flour/polypropylene injection molded composites. The poplar flour content was set at three different levels: 30%, 40% and 50%, the maleic anhydride polypropylene (MAPP) content was constant at 2%, and the nano-calcium carbonate content was set at four different levels: 0%, 1.5%, 3.0% and 4.5%. The materials were mixed in a co-rotating twins-crew extruder. Test samples were made by injection molding. The physical and mechanical properties were studied using X-ray diffraction and scanning electron microscopy. The results showed that the notched impact strength decreased, while the tensile and flexural strength, tensile and flexural moduli, hardness, water absorption and thickness swelling increased when the wood flour content increased from 30 to 50% and the nano-calcium carbonate level was 4.5% after 24 h. The X-ray diffraction spectra showed that an intercalation structure was created in the composite. The scanning electron microscopy images showed that the bonding surface between the matrix and the filler material increased with increasing nano-calcium carbonate and wood flour contents, resulting in stronger connections within the matrixes.
引用
收藏
页码:449 / 457
页数:9
相关论文
共 48 条
[1]  
[Anonymous], 2010, ASTM D256-10
[2]  
[Anonymous], 2010, D703110 ASTM
[3]  
[Anonymous], 2012, STANDARD PRACTICE IN
[4]  
[Anonymous], 2010, D224010 ASTM
[5]  
Ashenai G. F., 2013, MODARES MECH ENG, V13, P1
[6]  
ASTM, 2010, D79010 ASTM
[7]  
ASTM, 2010, ASTM D 638-10
[8]  
Blanchard V, 2011, BIORESOURCES, V6, P1219
[9]  
Chen H. T., 2004, WOOD FIBER SCI, V46, P1
[10]  
Chen HC, 2006, HOLZ ROH WERKST, V64, P172, DOI 10.1007/s00107-005-0072-x