Durable antimicrobial treatment of cotton fabrics using N-(2-hydroxy)propyl-3-trimethylammonium chitosan chloride and polycarboxylic acids

被引:74
作者
Kim, YH [1 ]
Nam, CW
Choi, JW
Jang, JH
机构
[1] Soongsil Univ, Dept Text Engn, Seoul 156743, South Korea
[2] Korea Inst Ind Technol, Kyonggi Do 429540, South Korea
[3] Kumoh Natl Univ Technol, Dept Text & Fash Engn, Kumi 730701, South Korea
关键词
crosslinking; fibers; FT-IR; mechanical properties;
D O I
10.1002/app.11845
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
N-(2-hydroxy)propyl-3-trimethylammonium chitosan chloride (HTCC), a water-soluble chitosan quaternary ammonium derivative, was used as an antimicrobial agent for cotton fabrics. HTCC has a lower minimum inhibition concentration (MIC) against Staphylococcus aureus, Klebsiella pneumoniae, and Escherichia coli compared to that of chitosan; however, the imparted antimicrobial activity is lost on laundering. Thus crosslinking agents were utilized to obtain a durable antimicrobial treatment by immobilizing HTCC. Several crosslinkers such as dimethyloldihydroxyethylene urea (DMDHEU), butanetetracarboxylic acid (BTCA), and citric acid (CA) were used with HTCC to improve the laundering durability of HTCC treatment by covalent bond formation between the crosslinker, HTCC and cellulose. The polycarboxylic acid treatment was superior to the DMDHEU treatment in terms of prolonged antimicrobial activity of the treated cotton after successive laundering. Also, the cotton treated with HTCC and BTCA showed improved durable press properties without excessive deterioration in mechanical strength or whiteness when compared to the citric acid treatment. With the addition of only 0.1% HTCC to BTCA solutions, the treated fabrics showed durable antimicrobial activity up to 20 laundering cycles. The wrinkle recovery angle and strength retention of the treated fabrics were not adversely affected with the addition of HTCC. Therefore, BTCA can be used with HTCC in one bath to impart durability of antimicrobial activity along with durable press properties to cotton fabric. (C) 2003 Wiley Periodicals.
引用
收藏
页码:1567 / 1572
页数:6
相关论文
共 18 条
[1]   NONPHOSPHORUS CATALYSTS FOR FORMALDEHYDE-FREE DP FINISHING OF COTTON WITH 1,2,3,4-BUTANETETRACARBOXYLIC ACID .1. AROMATIC N-HETEROCYCLIC COMPOUNDS [J].
CHOI, HM ;
WELCH, CM ;
MORRIS, N .
TEXTILE RESEARCH JOURNAL, 1993, 63 (11) :650-657
[2]   Durable press and antimicrobial finishing of cotton fabrics with a citric acid and chitosan treatment [J].
Chung, YS ;
Lee, KK ;
Kim, JW .
TEXTILE RESEARCH JOURNAL, 1998, 68 (10) :772-775
[3]  
Jang J., 2000, Fibers Polym, V1, P116, DOI DOI 10.1007/BF02875195
[4]  
KANG IS, 1997, TEXT RES J, V67, P865
[5]  
Kim YH, 1998, TEXT RES J, V68, P428
[6]   Durable press finish of cotton/polyester fabrics with 1,2,3,4-butanetetracarboxylic acid and sodium propionate [J].
Lee, ES ;
Kim, HJ .
JOURNAL OF APPLIED POLYMER SCIENCE, 2001, 81 (03) :654-661
[7]   Blend fibers of polyacrylonitrile and water-soluble chitosan derivative prepared from sodium thiocyanate solution [J].
Nam, CW ;
Kim, YH ;
Ko, SW .
JOURNAL OF APPLIED POLYMER SCIENCE, 2001, 82 (07) :1620-1629
[8]  
Nam CW, 1999, J APPL POLYM SCI, V74, P2258, DOI 10.1002/(SICI)1097-4628(19991128)74:9<2258::AID-APP15>3.3.CO
[9]  
2-0
[10]   Preparing chito-oligosaccharides as antimicrobial agents for cotton [J].
Seong, HS ;
Kim, JP ;
Ko, SW .
TEXTILE RESEARCH JOURNAL, 1999, 69 (07) :483-488