DETERMINATION OF THE CREEP-FATIGUE INTERACTION DIAGRAM FOR ALLOY 617

被引:0
|
作者
Wright, J. K. [1 ]
Carroll, L. J. [1 ]
Sham, T. -L. [2 ]
Lybeck, N. J. [1 ]
Wright, R. N. [1 ]
机构
[1] Idaho Natl Lab, Idaho Falls, ID 83402 USA
[2] Argonne Natl Lab, Argonne, IL USA
关键词
NICKEL-ALLOY; INCONEL-617;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Alloy 617 is the leading candidate material for an intermediate heat exchanger for the very high temperature reactor (VHTR). As part of evaluating the behavior of this material in the expected service conditions, creep fatigue testing was performed. The cycles to failure decreased compared to fatigue values when a hold time was added at peak tensile strain. At 850 degrees C, increasing the tensile hold duration continued to degrade the creep fatigue resistance, at least to the investigated strain controlled hold time of up to 60 minutes at the 0.3% strain range and 240 minutes at the 1.0% strain range. At 950 degrees C, the creep fatigue cycles to failure are not further reduced with increasing hold duration, indicating saturation occurs at relatively short hold times. The creep and fatigue damage fractions have been calculated and plotted on a creep fatigue interaction D-diagram. Test data from creep fatigue tests at 800 and 1000 degrees C on an additional heat of Alloy 617 are also plotted on the D-diagram.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Evaluation of creep-fatigue damage interaction in HK40 alloy
    Konosu, S.
    Koshimizu, T.
    Iijima, T.
    Maeda, K.
    Journal of Mechanical Design, Transactions Of the ASME, 1993, 115 (01): : 41 - 46
  • [32] On the biaxial thermal creep-fatigue behavior of Ni-base Alloy 617 at 950 °C
    Zhong, Yang
    Liu, Xiang
    Lan, Kuan-Che
    Lee, Hoon
    Tsang, D. K. L.
    Stubbins, James F.
    INTERNATIONAL JOURNAL OF FATIGUE, 2020, 139
  • [33] CREEP-FATIGUE INTERACTION ON TITANIUM-ALLOY VT-8
    JANOUSEK, M
    PUSKAR, A
    KOVOVE MATERIALY-METALLIC MATERIALS, 1994, 32 (04): : 273 - 281
  • [34] Creep-fatigue interaction of a high temperature (α+β) titanium alloy at room temperature
    Ramachandra, C
    Kashyap, KT
    Nanjundaswamy, GS
    Sridharan, NS
    Chatterji, B
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2000, 53 (03): : 277 - 282
  • [35] EVALUATION OF CREEP-FATIGUE DAMAGE INTERACTION IN HK40 ALLOY
    KONOSU, S
    KOSHIMIZU, T
    IIJIMA, T
    MAEDA, K
    JOURNAL OF MECHANICAL DESIGN, 1993, 115 (01) : 41 - 46
  • [36] Image-based creep-fatigue damage mechanism investigation of Alloy 617 at 950 °C
    Tahir, Fraaz
    Dahire, Sonam
    Liu, Yongming
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 679 : 391 - 400
  • [37] Assessment of modelling methodologies for prediction of high-temperature creep-fatigue behaviour of Alloy 617
    Douzian, G.
    Muransky, O.
    Kruzic, J. J.
    Wright, R. N.
    Payten, W.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2020, 187
  • [38] CREEP-FATIGUE LIFE AND DAMAGE EVALUATION OF NI-BASED ALLOY 617 AND ALLOY 740H
    Zhang, Shengde
    Takahashi, Yukio
    ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS: PROCEEDINGS FROM THE EIGHTH INTERNATIONAL CONFERENCE, 2016, 2016, : 149 - 160
  • [39] DAMAGE MODEL OF CREEP-FATIGUE INTERACTION
    JANSON, J
    ENGINEERING FRACTURE MECHANICS, 1979, 11 (02) : 397 - 403
  • [40] MATERIALS AND FABRICATION Creep and Creep-Fatigue Interaction Abstract
    Dogan, Bilal
    Nikbi, Kamran
    Ainsworth, Robert
    Takahashi, Yukio
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, PVP 2011, VOL 6, A AND B, 2012, : 117 - 117