Mixed-mode fracture analysis of composite bonded joints considering adhesives of different ductility

被引:22
作者
Santos, M. A. S. [1 ]
Campilho, R. D. S. G. [1 ,2 ]
机构
[1] Inst Politecn Porto, Inst Super Engn Porto, Dept Engn Mecan, Rua Dr Antonio Bernardino de Almeida 431, P-4200072 Oporto, Portugal
[2] INEGI Polo FEUP, Rua Dr Roberto Frias S-N, P-4200465 Oporto, Portugal
关键词
Bonded joint; Finite element analysis; Fracture mechanics; Mixed-mode fracture; DOUBLE-CANTILEVER BEAM; COHESIVE ZONE MODEL; R-CURVE; INTERLAMINAR FRACTURE; CRACK-GROWTH; SINGLE; TOUGHNESS; STRENGTH; TESTS; EPOXY;
D O I
10.1007/s10704-017-0219-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The use of adhesive joints in industrial applications has been increasing. To increase the confidence in the design of adhesive structures, it is important to be able to accurately predict their strength and fracture properties (critical strain energy release rate in tension, , and shear, . As in most cases loads induce mixed-mode (tension plus shear), it is of great importance the perception of fracture under these conditions, in which relates to the strain energy release rate in tension, , and shear, . This analysis allows choosing the best failure criterion to use in cohesive zone models, to predict the behaviour of bonded joints. This work presents an experimental and numerical study using the Single-Leg Bending (SLB) test on specimens bonded with three adhesives, to study and compare their mixed-mode fracture properties. For this purpose, data reduction methods were applied to estimate and that require the measurement of crack length (a) and methods using an equivalent crack length (. The analysis and comparison of and obtained during the experimental phase were addressed. Framing the obtained values in several fracture envelopes enable to select which failure criterion is more appropriate for each adhesive. Overall, a very good agreement was obtained between methods for the determination of and . Actually, apart from one of the methods that produced higher errors, the highest deviation to the -based method (considered as the most robust) was 9.3%, obtained for . In the numerical simulations it was possible to reproduce the observed behaviour of the experimental tests, with a positive validation of the chosen propagation criteria obtained from the experimental results.
引用
收藏
页码:55 / 71
页数:17
相关论文
共 61 条
  • [2] Fracture R-curve of a toughened epoxy adhesive as a function of irreversible degradation
    Ameli, A.
    Papini, M.
    Spelt, J. K.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (20): : 5105 - 5114
  • [3] [Anonymous], 2013, DOCUMENTATION
  • [4] [Anonymous], 2009, THESIS
  • [5] [Anonymous], 2000, ASTM STP
  • [6] Double cantilever beam testing of repaired carbon fibre composites
    Bader, MG
    Hamerton, I
    Hay, JN
    Kemp, M
    Winchester, S
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2000, 31 (06) : 603 - 608
  • [7] Belytschko T, 1999, INT J NUMER METH ENG, V45, P601, DOI 10.1002/(SICI)1097-0207(19990620)45:5<601::AID-NME598>3.0.CO
  • [8] 2-S
  • [9] Analytical and experimental investigations of crack propagation in adhesively bonded joints with the Mixed Mode Bending (MMB) test Part I: Macroscopic analysis & Digital Image Correlation measurements
    Ben Salem, N.
    Jumel, J.
    Budzik, M. K.
    Shanahan, M. E. R.
    Lavelle, F.
    [J]. THEORETICAL AND APPLIED FRACTURE MECHANICS, 2014, 74 : 209 - 221
  • [10] Cohesive zone modelling of nucleation, growth and coalesce of cavities
    Biel, A.
    Stigh, U.
    [J]. INTERNATIONAL JOURNAL OF FRACTURE, 2017, 204 (02) : 159 - 174