High Temperature Oxidation Behavior of New Martensitic Heat-Resistant Steel

被引:2
作者
Bao, Ziming [1 ]
Han, Renheng [1 ]
Zhu, Yanqing [1 ]
Li, Hong [1 ]
Li, Ning [1 ]
Tang, Ming [1 ]
Zhang, Hexin [1 ,2 ]
Zhao, Chengzhi [1 ,2 ]
机构
[1] Harbin Engn Univ, Coll Mat Sci & Chem Engn, 145 Nantong Ave, Harbin 150001, Heilongjiang, Peoples R China
[2] Harbin Engn Univ, Key Lab Superlight Mat & Surface Technol, Minist Educ, 145 Nantong Ave, Harbin 150001, Heilongjiang, Peoples R China
来源
MATERIALS SCIENCE-MEDZIAGOTYRA | 2022年 / 28卷 / 02期
关键词
heat-resistant steel; high temperature oxidation; morphology of oxide film; element distribution; OXIDE SCALE; MECHANICAL-PROPERTIES; ALLOY; EVOLUTION; MICROSTRUCTURE; CORROSION; SILICON; METALS; PHASE; WATER;
D O I
10.5755/j02.ms.27438
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The research focuses on the high temperature oxidation resistance of martensitic heat-resistant steel. A new type of martensitic heat-resistant steel was developed with the addition of Al and Cu, and the oxidation behavior of the new martensitic heat-resistant steel at 650 degrees C and 700 degrees C was analyzed. The high temperature oxidation kinetics curves of new martensitic heat-resistant steel at 650 degrees C and 700 degrees C were determined and plotted by cyclic oxidation experiment and discontinuous weighing method. XRD technique was applied to qualitatively analyze the surface oxide of the material after oxidation. The surface and cross-section morphology of the material were observed by field emission scanning electron microscope (SEM) and energy dispersive spectrometer (EDS), and the oxidation mechanism at high temperature was analyzed. The results show that the oxide film can be divided into two layers after oxidation at 650 degrees C for 200 h. The outer oxide film is mainly composed of Fe and Cu oxides, and the inner oxide film is mainly composed of Al2O3, SiO2 and Cr2O3. After oxidation at 700 degrees C for 200 h, the outer layer is mainly composed of Fe, Cu, Mn oxides, and the inner layer is mainly composed of Cr, Al and Si oxides. The addition of a small amount of Cu promotes the diffusion of Al and Si elements, facilitates the formation of Al2O3 and SiO2, and improves the high-temperature oxidation resistance of martensitic heat-resistant steel.
引用
收藏
页码:164 / 170
页数:7
相关论文
共 38 条
[1]   High temperature oxidation of Fe-Al and Fe-Cr-Al alloys: The role of Cr as a chemically active element [J].
Airiskallio, E. ;
Nurmi, E. ;
Heinonen, M. H. ;
Vayrynen, I. J. ;
Kokko, K. ;
Ropo, M. ;
Punkkinen, M. P. J. ;
Pitkanen, H. ;
Alatalo, M. ;
Kollar, J. ;
Johansson, B. ;
Vitos, L. .
CORROSION SCIENCE, 2010, 52 (10) :3394-3404
[2]   A Study of Microstructure and Mechanical Properties of Grade 91 Steel A-TIG Weld Joint [J].
Arivazhagan, B. ;
Vasudevan, M. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (12) :3708-3716
[3]   Thermal oxidation kinetics and oxide scale adhesion of Fe-15Cr alloys as a function of their silicon content [J].
Bamba, G. ;
Wouters, Y. ;
Galerie, A. ;
Charlot, F. ;
Dellali, A. .
ACTA MATERIALIA, 2006, 54 (15) :3917-3922
[4]   Alloy design strategies for promoting protective oxide scale formation [J].
Brady, MP ;
Gleeson, B ;
Wright, IG .
JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 2000, 52 (01) :16-21
[5]   MECHANISM OF TRANSPORT OF MATTER THROUGH SCALES DURING OXIDATION OF METALS AND ALLOYS [J].
BRUCKMAN, A .
CORROSION SCIENCE, 1967, 7 (01) :51-&
[6]   Strengthening effect of Cu-rich phase precipitation in 18Cr9Ni3CuNbN austenitic heat-resisting steel [J].
Chi, Chengyu ;
Yu, Hongyao ;
Dong, Jianxin ;
Xie, Xishan ;
Cui, Zhengqiang ;
Chen, Xiaofang ;
Lin, Fusheng .
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2011, 24 (02) :141-147
[7]   The internal oxidation of ternary alloys I: The single oxidation of the most-reactive component under low oxidant pressures [J].
Gesmundo, F ;
Niu, Y .
OXIDATION OF METALS, 2003, 60 (5-6) :347-370
[8]  
Hong L., 2019, PROPERTIES HIGH TEMP, V25, P394
[9]   Oxidation of AISI 304 and AISI 439 stainless steels [J].
Huntz, A. M. ;
Reckmann, A. ;
Haut, C. ;
Severac, C. ;
Herbst, M. ;
Resende, F. C. T. ;
Sabioni, A. C. S. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 447 (1-2) :266-276
[10]   Effect of silicon on the oxidation resistance of 9% Cr steels [J].
Huntz, AM ;
Bague, V ;
Beauplé, G ;
Haut, C ;
Sévérac, C ;
Lecour, P ;
Longaygue, X ;
Ropital, F .
APPLIED SURFACE SCIENCE, 2003, 207 (1-4) :255-275