Sintering aids in the consolidation of boron carbide (B4C) by the Plasma Pressure Compaction (P2C) method

被引:26
|
作者
Klotz, BR [1 ]
Cho, KC [1 ]
Dowding, RJ [1 ]
机构
[1] USA, Res Lab, Weapons Mat Res Directorate, AMSRD,ARL,WM,MB, Aberdeen Proving Ground, MD 21005 USA
关键词
boron carbide; powder consolidation; plasma pressure compaction; sintering aids; alumina; titanium diboride; carbon;
D O I
10.1081/LMMP-200028083
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Boron carbide (B4C) powder has been densified by a novel method of powder consolidation known as Plasma Pressure Compaction ((PC)-C-2). The (PC)-C-2 technique allows for rapid consolidation of powder by Joule heating of the powder bed. Powder is placed in graphite dies, and uniaxial pressure and low-voltage, high-amperage (10V, 5000 amps maximum) direct current are applied to achieve densification. Pure B4C powder was consolidated at lower temperature and hold time to densities equal to those achieved by conventional hot pressing. With the addition of a small amount of alumina (Al2O3) as a sintering aid, densities as high as 97% theoretical were attained.
引用
收藏
页码:631 / 639
页数:9
相关论文
共 50 条
  • [1] Spark plasma sintering of boron carbide (B4C): From characterisation to finite element modeling of sintering
    Grippi, Thomas
    Torresani, Elisa
    Maximenko, Andrii L.
    Olevsky, Eugene A.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (15)
  • [2] On melting of B4C boron carbide under pressure
    V. A. Mukhanov
    P. S. Sokolov
    V. L. Solozhenko
    Journal of Superhard Materials, 2012, 34 : 211 - 213
  • [3] On melting of B4C boron carbide under pressure
    Mukhanov, V. A.
    Sokolov, P. S.
    Solozhenko, V. L.
    JOURNAL OF SUPERHARD MATERIALS, 2012, 34 (03) : 211 - 213
  • [4] Tribological Characterization of SiC and B4C Manufactured by Plasma Pressure Compaction
    Rubino, Felice
    Pisaturo, Mario
    Senatore, Adolfo
    Carlone, Pierpaolo
    Sudarshan, Tirumalai S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (11) : 5648 - 5659
  • [5] Tribological Characterization of SiC and B4C Manufactured by Plasma Pressure Compaction
    Felice Rubino
    Mario Pisaturo
    Adolfo Senatore
    Pierpaolo Carlone
    Tirumalai S. Sudarshan
    Journal of Materials Engineering and Performance, 2017, 26 : 5648 - 5659
  • [6] Temperature and pressure dependences of the elastic properties of ceramic boron carbide (B4C)
    S. P. Dodd
    G. A. Saunders
    B. James
    Journal of Materials Science, 2002, 37 : 2731 - 2736
  • [7] COMPRESSION AND ASSOCIATED PROPERTIES OF BORON CARBIDE (B4C)
    Ciezak, J. A.
    Dandekar, D. P.
    SHOCK COMPRESSION OF CONDENSED MATTER - 2009, PTS 1 AND 2, 2009, 1195 : 1287 - 1290
  • [8] The effect of sintering parameters on spark plasma sintering of B4C
    Asadikiya, Mohammad
    Zhang, Cheng
    Rudolf, Christopher
    Boesl, Benjamin
    Agarwal, Arvind
    Zhong, Yu
    CERAMICS INTERNATIONAL, 2017, 43 (14) : 11182 - 11188
  • [9] Reactive Synthesis of B4C–CrB2, B4C–TiB2, AND B4C–TiCrB2 Heterophase Ceramics by Spark Plasma Sintering
    T. M. Kutran
    M. V. Zamula
    B. A. Pokhylko
    O. V. Shyrokov
    V. G. Kolesnichenko
    V. V. Kovalchuk
    A. V. Stepanenko
    H. Yu. Borodianska
    Powder Metallurgy and Metal Ceramics, 2023, 61 : 522 - 540
  • [10] In situ synthesis and sintering of B4C/ZrB2 composites from B4C and ZrH2 mixtures by spark plasma sintering
    Rehman, Sahibzada Shakir
    Ji, Wei
    Fu, Zhengyi
    Wang, Weimin
    Wang, Hao
    Asif, Muhammad
    Zhang, Jinyong
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2015, 35 (04) : 1139 - 1145