摘要
The wetting behavior and interface interaction in the CaF2/Me and NaCl/Me systems were studied using the sessile drop method. It was observed that liquid Bi, In, Sn and Ga do not wet the CaF2 and NaCl substrates at 1000 K and liquid Cu does not wet the CaF2 substrate in the 1423-1573 K temperature range. Nevertheless, different spreading behavior was observed during experiments. For the CaF2/Me systems, at 1000 K, the contact angle remains constant with time, while for the NaCl/Me systems, a non-monotonic spreading behavior was detected. For these systems the contact angle increases initially and then rapidly decreases. For the CaF2/Cu system at 1423 K the contact angle remains constant, while it increases with time at 1573 K. It was established that the wetting behavior is attributed to the evaporation of the solid substrate, which leads to the formation of a neck-shape interface. The experimental results were well accounted for by a model, which considered the geometrical characteristic of the metal/ceramic interface and thermo-physical properties of the metals and the substrates. (c) 2007 Elsevier Masson SAS. All rights reserved.
引用
收藏
页码:338 / 343
页数:6
相关论文
共 15 条
[1]  
BARZILAI S, IN PRESS ALLOYS COMP, DOI DOI 10.1016/J.JALLCOM.2006.11.213
[2]  
BARZILAI S, 2006, ADV SCI TECHNOL, V45, P1532
[3]   Dewetting modes of thin metallic films: Nucleation of holes and spinodal dewetting [J].
Bischof, J ;
Scherer, D ;
Herminghaus, S ;
Leiderer, P .
PHYSICAL REVIEW LETTERS, 1996, 77 (08) :1536-1539
[4]   WETTING OF ALUMINIUM OXIDE BY MOLTEN ALUMINIUM AND OTHER METALS [J].
CHAMPION, JA ;
KEENE, BJ ;
SILLWOOD, JM .
JOURNAL OF MATERIALS SCIENCE, 1969, 4 (01) :39-&
[5]  
Eustathopoulos N., 1999, Wettability at High Temperatures
[6]  
Iida T., 1988, PHYS PROPERTIES LIQU
[7]  
KRASOVSKY VP, 2001, T JWRI, V30, P61
[8]   The evaporation, condensation and reflection of molecules and the mechanism of adsorption [J].
Langmuir, I .
PHYSICAL REVIEW, 1916, 8 (02) :149-176
[9]   Aluminium-alumina interface morphology and thermodynamics from dewetting experiments [J].
Levi, G ;
Kaplan, WD .
ACTA MATERIALIA, 2003, 51 (10) :2793-2802
[10]   The nonwettability behaviour of solid substrates in contact with chemical active reach Ti-, Zr- and Hf-liquid alloys [J].
Naidich, Y ;
Krasovsky, V .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (08) :683-685