Hydrogen bulk retention in graphite and kinetics of diffusion

被引:37
作者
Atsumi, H [1 ]
机构
[1] Kinki Univ, Dept Nucl Engn, Fac Sci & Engn, Higashiosaka, Osaka 5778502, Japan
基金
日本学术振兴会;
关键词
D O I
10.1016/S0022-3115(02)01069-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Molecular hydrogen absorption into graphite has been studied in order to obtain information on the 'true' hydrogen diffusion coefficient in graphite, oxygen effect and the mechanism of hydrogen trapping, which should be important issues on estimating hydrogen retention and recycling in plasma facing graphite and CFC. Hydrogen may permeate into a filler grain in the form of hydrogen molecules, diffuse through crystallite boundaries, and may finally be trapped as hydrogen atoms at the edge surface of a crystallite. The diffusion coefficient can be given as D.(m(2)/s) 3.3 x 10(-10)(-1.3 eV/kT), when the trapping effect does not exist. The simulation with mass balance equations can reproduce change of apparent diffusion coefficients. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:1466 / 1470
页数:5
相关论文
共 31 条
[1]   Hydrogen absorption process into graphite and carbon materials [J].
Atsumi, H ;
Iseki, M .
JOURNAL OF NUCLEAR MATERIALS, 2000, 283 :1053-1056
[2]   TRAPPING AND DETRAPPING OF HYDROGEN IN CARBON-BASED MATERIALS EXPOSED TO HYDROGEN GAS [J].
ATSUMI, H ;
ISEKI, M ;
SHIKAMA, T .
JOURNAL OF NUCLEAR MATERIALS, 1994, 212 :1478-1482
[3]  
ATSUMI H, 1992, J NUCL MATER, V191, P368
[4]   ABSORPTION AND DESORPTION OF DEUTERIUM ON GRAPHITE AT ELEVATED-TEMPERATURES [J].
ATSUMI, H ;
TOKURA, S ;
MIYAKE, M .
JOURNAL OF NUCLEAR MATERIALS, 1988, 155 :241-245
[5]  
ATSUMI H, 1996, J NUCL MATER B, V237, P1128
[6]   Present status and future prospect of the ITER project [J].
Aymar, R .
JOURNAL OF NUCLEAR MATERIALS, 1998, 258 :56-64
[7]   THE RETENTION OF DEUTERIUM AND TRITIUM IN POCO AXF-5Q GRAPHITE [J].
CAUSEY, RA ;
BASKES, MI ;
WILSON, KL .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1986, 4 (03) :1189-1192
[8]   HYDROGEN DIFFUSION AND SOLUBILITY IN PYROLYTIC CARBON [J].
CAUSEY, RA ;
ELLEMAN, TS ;
VERGHESE, K .
CARBON, 1979, 17 (04) :323-328
[9]   THE INTERACTION OF TRITIUM WITH GRAPHITE AND ITS IMPACT ON TOKAMAK OPERATIONS [J].
CAUSEY, RA .
JOURNAL OF NUCLEAR MATERIALS, 1989, 162 :151-161
[10]   Deuterium trapping in deep traps of differently oriented pyrolytic graphite exposed to D2 gas at 1473 K [J].
Chernikov, VN ;
Wampler, WR ;
Zakharov, AP ;
Gorodetsky, AE .
JOURNAL OF NUCLEAR MATERIALS, 1999, 264 (1-2) :180-197