Bond strength of glass fiber-reinforced polymer bars in concrete after exposure to elevated temperatures

被引:32
作者
El-Gamal, Sherif [1 ]
机构
[1] Sultan Qaboos Univ, Dept Civil & Architectural Engn, Muscat 123, Oman
关键词
Bond; glass fiber-reinforced polymer bars; concrete; temperature; interface; pullout test; BEHAVIOR; FRP; PERFORMANCE; REBARS;
D O I
10.1177/0731684414555408
中图分类号
TB33 [复合材料];
学科分类号
摘要
This paper presents the test results of an experimental study to investigate the effect of elevated temperatures on the bond properties of glass fiber-reinforced polymer bars in concrete. For this purpose, a total of 39 pullout specimens with glass fiber-reinforced polymer bars were cast for bond strength tests. In addition to the laboratory temperature, specimens were exposed to heating regimes of 100, 200, 300 and 350? for a period of 1, 2 or 3h. The test results are presented in terms of bond strength, bond-slip relationship, and mode of failure. All specimens failed by shearing of the concrete corbels surrounding the bars and almost no damage was seen in the glass fiber-reinforced polymer bars. The results showed that the bond strength decreased as the temperature or exposure period increased. Reductions of about 20% of the original bond strength were recorded after exposure to 100 and 200? for 3h. Significant reductions of about 50% in the bond strength were recorded after exposure to 350? for periods of 2 and 3h. A modification to the ACI (American Concrete Institute) and CEB-FIP (Comite Euro-International du Beton-Federation Internationale de la Precontrainte) equations was developed to consider the effect of elevated temperatures and it showed good agreement with test results.
引用
收藏
页码:2151 / 2163
页数:13