Reaction Behaviour between Cerium Ferroalloy and Molten Steel during Rare Earth Treatment in the Ultra-low Carbon Al-killed Steel

被引:7
作者
Wang, Min [1 ]
Gao, Shuai [1 ]
Li, Xin [1 ]
Wu, Gui-xuan [2 ,3 ]
Xing, Li-dong [1 ]
Wang, Hao [1 ,4 ]
Zhi, Jian-guo [4 ]
Bao, Yan-ping [1 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met, Xueyuan Rd 30, Beijing 100083, Peoples R China
[2] GTT Technol, Kaiserstr 103, D-52134 Herzogenrath, Germany
[3] Forschungszentrum Julich, Inst Energy & Climate Res, Microstruct & Properties Mat IEK 2, Leo Brandt Str 1, D-52425 Julich, Germany
[4] Baotou Iron & Steel Grp Corp, Baotou Nei Mongol 014010, Peoples R China
关键词
cerium ferroalloy; rare earth treatment; ultra-low carbon Al-killed steel; reaction interface; inclusions transformation; THERMODYNAMIC ASSESSMENT; INCLUSION MODIFICATION; HOT DUCTILITY; IMPURITY TIN; LA; CE; EVOLUTION; CORROSION; ELEMENTS; ZN;
D O I
10.2355/isijinternational.ISIJINT-2020-678
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this work, the melting process and reaction behaviour of cerium ferroalloy in the liquid ultra-low carbon interstitial free steel was investigated through a special designed hot crucible experiment using standard metallographic techniques including SEM, EDS, XRF, and XRD in combination with the thermodynamic software FactSage 7.2. The evolution mechanism of cerium-containing phases in the cerium ferroalloy during the melting process was proposed. The cerium-containing phases stretched and migrated along the direction of heat flow, in further the arms of the network structures became thinner and finally dissolved into the molten steel. It was concluded that the thinner of network structures' arms, the higher of the Ce content in cerium-containing phases. During the melting process, the cerium content in the cerium-enriched phase was increased from 43.9 wt% in the matrix of the cerium ferroalloy to 90.44 wt% in the reaction zone, and the average width of the network arms was decreased from 18 mu m to 2 mu m accordingly. The main reaction products in the interface among cerium ferroalloy, molten steel, and slag were Ce2O3 and CeAlO3.
引用
收藏
页码:1524 / 1531
页数:8
相关论文
共 35 条
  • [1] Effect of CeO2 on heat transfer and crystallization behavior of rare earth alloy steel mold fluxes
    Cai, Ze-yun
    Song, Bo
    Li, Long-fei
    Liu, Zhen
    Cui, Xiao-kang
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2019, 26 (05) : 565 - 572
  • [2] [曹战民 Cao Zhanmin], 2008, [稀有金属, Chinese Journal of Rare Metals], V32, P216
  • [3] Effect of rare earth and alloying elements on the thermal conductivity of austenitic medium manganese steel
    Chen, Shao-chun
    Ye, Hong-xiang
    Lin, Xin-qiang
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2017, 24 (06) : 670 - 674
  • [4] Effect of Rare Earth Element La on Texture and Inclusion of Non-oriented Electrical Steel Produced by Thin Slab Casting and Rolling Process
    Fan, Lifeng
    Zhu, Rong
    He, Jianzhong
    Lu, Bin
    [J]. ISIJ INTERNATIONAL, 2018, 58 (12) : 2348 - 2353
  • [5] Characterization Transformation of Inclusions Using Rare Earth Ce Treatment on Al-Killed Titanium Alloyed Interstitial Free Steel
    Gao, Shuai
    Wang, Min
    Guo, Jian-long
    Wang, Hao
    Zhi, Jian-guo
    Bao, Yan-ping
    [J]. STEEL RESEARCH INTERNATIONAL, 2019, 90 (10)
  • [6] Microstructures and thermal fatigue behavior of Cr-Ni-Mo hot work die steel modified by rare earth
    Guan, QF
    Jiang, QC
    Fang, JR
    Jiang, H
    [J]. ISIJ INTERNATIONAL, 2003, 43 (05) : 784 - 789
  • [7] Effect of Cerium on the Behavior of Inclusions in H13 Steel
    Huang, Yu
    Cheng, Guoguang
    Li, Shijian
    Dai, Weixing
    [J]. STEEL RESEARCH INTERNATIONAL, 2018, 89 (12)
  • [8] Cathodoluminescence Analysis of Nonmetallic Inclusions in Steel Deoxidized and Desulfurized by Rare-Earth Metals (La, Ce, Nd)
    Imashuku, Susumu
    Wagatsuma, Kazuaki
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2020, 51 (01): : 79 - 84
  • [9] Effects of cerium on the compositional variations in and around inclusions and the initiation and propagation of pitting corrosion in hyperduplex stainless steels
    Jeon, Soon-Hyeok
    Kim, Soon-Tae
    Choi, Min-Seok
    Kim, Ji-Soo
    Kim, Kwang-Tae
    Park, Yong-Soo
    [J]. CORROSION SCIENCE, 2013, 75 : 367 - 375
  • [10] Katsumata A., 2002, Iron Steelmak, V29, P51