Tailoring microstructure and microhardness of Zn-1wt.%Mg-(0.5wt.%Mn, 0.5wt.%Ca) alloys by solidification cooling rate

被引:15
|
作者
Vida, Talita A. [1 ]
Silva, Cassio A. P. [1 ]
Lima, Thiago S. [1 ]
Cheung, Noe [1 ]
Brito, Crystopher [2 ]
Garcia, Amauri [1 ]
机构
[1] Univ Campinas UNICAMP, Dept Mfg & Mat Engn, BR-13083860 Campinas, SP, Brazil
[2] Sao Paulo State Univ UNESP, Campus Sao Joao da Boa Vista, BR-13876750 Sao Joao Da Boa Vista, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Zn-Mg-(Ca; Mn) alloys; solidification; cooling rate; microstructure; microhardness; ZN-BASED ALLOYS; MECHANICAL-PROPERTIES; THERMAL PARAMETERS; LENGTH SCALE; MG ALLOYS; ALUMINUM; GROWTH; ZINC; STABILITY; CORROSION;
D O I
10.1016/S1003-6326(21)65559-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Biodegradable Zn-based alloys, particularly Zn-Mg alloys with the addition of alloying elements, have been intensively investigated aiming to improve both mechanical properties and corrosion behavior. Since such properties are strongly dependent on the alloy microstructure, any evaluation should commence on understanding the conditions influencing its formation. In this study, the effect of the solidification cooling rate on the microstructural evolution of Zn-1wt.%Mg-(0.5wt.%Ca, 0.5wt.%Mn) alloys during transient solidification was investigated. The results show that the microstructures of both alloys have three phases in common:eta-Zn dendritic matrix, intermetallic compounds (IMCs) Zn11Mg2, and Zn2Mg in the eutectic mixture. MnZn9 and two Ca-bearing phases (CaZn11 and CaZn13) are associated with Mn and Ca additions, respectively. These additions are shown to refine the dendritic matrix and the eutectic mixture as compared to the Zn-1wt.%Mg alloy. A correlation between cooling rate, dendritic or eutectic spacings was developed, thus permitting experimental growth laws to be proposed. Additionally, hardness tests were performed to evaluate the effects of additions of Ca and Mn. Experimental correlations between Vickers microhardness and secondary dendritic spacings were proposed, showing that the microstructural refinement and characteristic Ca and Mn based IMCs induce an increase in hardness as compared to the binary alloy.
引用
收藏
页码:1031 / 1048
页数:18
相关论文
共 50 条
  • [41] A comparative study on the effect of 0.5 wt% Ca or Ce on the microstructure, texture, and mechanical properties of the hot-rolled Mg-4Li alloy
    Zhang, Songlin
    Fan, Yuheng
    Zhao, Hongliang
    Dong, Xianglei
    Guo, Chunwen
    Zhang, Shuya
    Weng, Kangrong
    Xiao, Yang
    MATERIALS TODAY COMMUNICATIONS, 2024, 39
  • [42] Microstructure and mechanical properties of Mg-5Zn-3.5Sn-1Mn-0.5Ca-0.5Cu alloy
    Wang, Cong
    Luo, Tianjiao
    Liu, Yunteng
    Lin, Tao
    Yang, Yuansheng
    MATERIALS CHARACTERIZATION, 2019, 147 : 406 - 413
  • [43] Homogenization-induced age-hardening behavior and room temperature mechanical properties of Mg-4Zn-0.5Ca-0.16Mn (wt%) alloy
    Duley, Partha
    Sanyal, Souriddha
    Bandyopadhyay, T. K.
    Mandal, Sumantra
    MATERIALS & DESIGN, 2019, 164
  • [44] Effects of 0.5 wt.% Nd Addition on the Microstructure and Mechanical Properties of As-Extruded and Aged Mg-6Al-3Sn-2Zn Alloys
    Wang, Sen
    Gao, Fu-Hao
    Lv, Bin-Jiang
    Cui, Ning
    Guo, Feng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (06) : 2635 - 2645
  • [45] Effects of 0.5 wt.% Nd Addition on the Microstructure and Mechanical Properties of As-Extruded and Aged Mg-6Al-3Sn-2Zn Alloys
    Sen Wang
    Fu-Hao Gao
    Bin-Jiang Lv
    Ning Cui
    Feng Guo
    Journal of Materials Engineering and Performance, 2023, 32 : 2635 - 2645
  • [46] Effect of Sn addition on the microstructure and mechanical properties of Mg-6Zn-1Mn (wt.%) alloy
    Qi, Fugang
    Zhang, Dingfei
    Zhang, Xiaohua
    Xu, Xingxing
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 585 : 656 - 666
  • [47] Role of hydrogen evolution rate in determining the corrosion rate of extruded Mg-5Sn-(1-4 wt%)Zn alloys
    Ha, Heon-Young
    Kang, Jun-Yun
    Yim, Chang Dong
    Yang, Jie
    You, Bong Sun
    CORROSION SCIENCE, 2014, 89 : 275 - 285
  • [48] Microstructure evolution of Zn-0.2Mg-0.8Mn(wt-%) alloys with different initial textures during room-temperature compression
    Wang, Liqing
    Lou, Dongfang
    Sun, Shineng
    Ren, Yuping
    Qin, Gaowu
    Bai, Peikang
    Zhao, Zhanyong
    MATERIALS SCIENCE AND TECHNOLOGY, 2022, 38 (16) : 1368 - 1375
  • [49] Tailoring the Mechanical and Degradation Performance of Mg-2.0Zn-0.5Ca-0.4Mn Alloy Through Microstructure Design
    Mostaed, Ehsan
    Sikora-Jasinska, Malgorzata
    Wang, Lifei
    Mostaed, Ali
    Reaney, Ian M.
    Drelich, Jaroslaw W.
    JOM, 2020, 72 (05) : 1880 - 1891
  • [50] Fabrication of a high strength Mg-11Gd-4.5Y-1Nd-1.5Zn-0.5Zr (wt%) alloy by thermomechanical treatments
    Yu, Zijian
    Huang, Yuanding
    Qiu, Xin
    Wang, Guanfu
    Meng, Fanzhi
    Hort, Norbert
    Meng, Jian
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 622 : 121 - 130