Tailoring microstructure and microhardness of Zn-1wt.%Mg-(0.5wt.%Mn, 0.5wt.%Ca) alloys by solidification cooling rate

被引:15
|
作者
Vida, Talita A. [1 ]
Silva, Cassio A. P. [1 ]
Lima, Thiago S. [1 ]
Cheung, Noe [1 ]
Brito, Crystopher [2 ]
Garcia, Amauri [1 ]
机构
[1] Univ Campinas UNICAMP, Dept Mfg & Mat Engn, BR-13083860 Campinas, SP, Brazil
[2] Sao Paulo State Univ UNESP, Campus Sao Joao da Boa Vista, BR-13876750 Sao Joao Da Boa Vista, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Zn-Mg-(Ca; Mn) alloys; solidification; cooling rate; microstructure; microhardness; ZN-BASED ALLOYS; MECHANICAL-PROPERTIES; THERMAL PARAMETERS; LENGTH SCALE; MG ALLOYS; ALUMINUM; GROWTH; ZINC; STABILITY; CORROSION;
D O I
10.1016/S1003-6326(21)65559-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Biodegradable Zn-based alloys, particularly Zn-Mg alloys with the addition of alloying elements, have been intensively investigated aiming to improve both mechanical properties and corrosion behavior. Since such properties are strongly dependent on the alloy microstructure, any evaluation should commence on understanding the conditions influencing its formation. In this study, the effect of the solidification cooling rate on the microstructural evolution of Zn-1wt.%Mg-(0.5wt.%Ca, 0.5wt.%Mn) alloys during transient solidification was investigated. The results show that the microstructures of both alloys have three phases in common:eta-Zn dendritic matrix, intermetallic compounds (IMCs) Zn11Mg2, and Zn2Mg in the eutectic mixture. MnZn9 and two Ca-bearing phases (CaZn11 and CaZn13) are associated with Mn and Ca additions, respectively. These additions are shown to refine the dendritic matrix and the eutectic mixture as compared to the Zn-1wt.%Mg alloy. A correlation between cooling rate, dendritic or eutectic spacings was developed, thus permitting experimental growth laws to be proposed. Additionally, hardness tests were performed to evaluate the effects of additions of Ca and Mn. Experimental correlations between Vickers microhardness and secondary dendritic spacings were proposed, showing that the microstructural refinement and characteristic Ca and Mn based IMCs induce an increase in hardness as compared to the binary alloy.
引用
收藏
页码:1031 / 1048
页数:18
相关论文
共 50 条
  • [31] Microstructure, Mechanical Properties, Electric and Thermal Conductivity of the As-Extruded Al-x(1.0 wt.% Zn+0.5 wt.% Cu) Alloys (x=1, 2 and 4)
    Kim, Yong-Ho
    Yoo, Hyo-Sang
    Son, Hyeon-Taek
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2020, 20 (07) : 4248 - 4252
  • [32] The relationship between microstructure and corrosion behaviors of Mg-3Y-xNd alloys (x=0.5, 1.0, 1.5 wt%)
    Jiang, Q. -T.
    Li, J. -R.
    Ma, X. -M.
    Li, Y. -T.
    Hou, B. -R.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2016, 67 (08): : 876 - 881
  • [33] Modelling corrosion rate of biodegradable magnesium-based alloys: The case study of Mg-Zn-RE-xCa (x=0, 0.5, 1.5, 3 and 6 wt%) alloys
    Bakhsheshi-Rad, Hamid Reza
    Abdellahi, Majid
    Hamzah, Esah
    Ismail, Ahmad Fauzi
    Bahmanpour, Maryam
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 687 : 630 - 642
  • [34] Effects of cooling rate on bio-corrosion resistance and mechanical properties of Mg-1Zn-0.5Ca casting alloy
    Wang, Li-dong
    Li, Xue-song
    Wang, Chao
    Wang, Li-min
    Cao, Zhan-yi
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2016, 26 (03) : 704 - 711
  • [35] Investigating the mechanical properties and corrosion resistance of extruded Mg-1Zn-xCaO (x=0, 0.5, 1.0 wt%) materials
    Shen, Guangxin
    Lyu, Shaoyuan
    Yu, Qianqian
    Wang, Xuewei
    Chen, Minfang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [36] Effect of phosphate post-treatment on corrosion behavior of cerium-based conversion coated Mg-4.0Y-4.0Zn-0.5Zr-0.2Ca (wt.%) alloys
    Kamde, Meeta Ashok
    Mahton, Yogendra
    Kumar, Ankit
    Prakash, N. Surya
    Roy, Mangal
    Basu, Anindya
    Saha, Partha
    MATERIALS CHEMISTRY AND PHYSICS, 2024, 314
  • [37] Effect of cooling rate on microstructure, mechanical and wear properties of Mg-2Zn and Mg-2Zn-1Mn alloys
    Elen, Levent
    Elen, Nurhan Cevik
    CANADIAN METALLURGICAL QUARTERLY, 2025, 64 (01) : 61 - 76
  • [38] The Microstructure and Mechanical Properties of As-cast Mg-10Gd-3Y-xZn-0.6Zr (x=0, 0.5, 1 and 2 wt%) Alloys
    Ding, Zhibing
    Lu, Ruopeng
    Zhao, Yuhong
    Hou, Hua
    Cheng, Peng
    Bu Zhiqiang
    Zhang, Peilin
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2018, 21 (05):
  • [39] The effect of homogenization on microstructures and mechanical properties of Mg-7Gd-3Y-1Nd-xZn-0.5Zr (x=0.5, 1 and 2 wt.%) alloys
    Li, M.
    Zhang, K.
    Du, Z. W.
    Li, X. G.
    Li, Y. J.
    Ma, M. L.
    Shi, G. L.
    Yuan, J. W.
    Li, T.
    Liu, J. B.
    MATERIALS CHARACTERIZATION, 2015, 109 : 66 - 72
  • [40] Formation and characterization of microstructure of as-cast Mg-6Gd-4Y-xZn-0.5Zr (x=0.3, 0.5 and 0.7 wt.%) alloys
    Wu, Y. J.
    Xu, C.
    Zheng, F. Y.
    Peng, L. M.
    Zhang, Y.
    Ding, W. J.
    MATERIALS CHARACTERIZATION, 2013, 79 : 93 - 99