Forming limit diagrams for AA5083 under SPF and QPF conditions

被引:14
|
作者
Kulas, Mary-Anne [1 ]
Krajewski, Paul E. [2 ]
Bradley, John R. [2 ]
Taleff, Eric M. [3 ]
机构
[1] Teuchos, Aerosp Div, Elancourt, Ile De France, France
[2] Gen Motors R&D Ctr, Warren, MI 48090 USA
[3] Univ Texas Austin, Dept Mech Engn, Austin, TX USA
来源
关键词
superplastic; quick plastic; SPF; QPF; AA5083; formability; FLD;
D O I
10.4028/www.scientific.net/MSF.551-552.129
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Forming Limit Diagrams (FLD's) for AA5083 aluminum sheet were established under both Superplastic Forming (SPF) and Quick Plastic Forming (QPF) conditions. SPF conditions consisted of a strain rate of 0.0001/s at 500 degrees C, while QPF conditions consisted of a strain rate of 0.01/s at 450 degrees C. The forming limit diagrams were generated using uniaxial tension, biaxial bulge, and plane strain bulge testing. Forming limits were defined using two criteria: (1) macroscopic fracture and (2) greater than 2% cavitation. Very little difference was observed between the plane strain limits in the SPF and QPF conditions indicating comparable formability between the two processes with a commercial grade AA5083 material.
引用
收藏
页码:129 / +
页数:2
相关论文
共 50 条
  • [1] Microstructural characterization of superplastic forming (SPF) AA5083 aluminum sheet
    Kim, S
    Balogh, MP
    Waldo, RA
    ADVANCES IN SUPERPLASTICITY AND SUPERPLASTIC FORMING, 2004, : 139 - 148
  • [2] Formability Characteristics of AA5083 Sheets Under Hot Forming Conditions
    Bruschi, Stefania
    Ghiotti, Andrea
    Michieletto, Francesco
    SHEET METAL 2013, 2013, 549 : 356 - 363
  • [3] Forming-limit diagrams for hot-forming of AA5083 aluminum sheet: Continuously cast material
    Kulas, Maty-Anne
    Krajewski, Paul E.
    Bradley, John R.
    Taleff, Eric M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2007, 16 (03) : 308 - 313
  • [4] Forming-Limit Diagrams for Hot-Forming of AA5083 Aluminum Sheet: Continuously Cast Material
    Mary-Anne Kulas
    Paul E. Krajewski
    John R. Bradley
    Eric M. Taleff
    Journal of Materials Engineering and Performance, 2007, 16 : 308 - 313
  • [5] Forming limit diagram of a superplastic formable AA5083 aluminum alloy
    Vulcan, M
    Siegert, K
    ADVANCES IN SUPERPLASTICITY AND SUPERPLASTIC FORMING, 2004, : 351 - 360
  • [6] Effect of Equal Biaxial Pre-Strain on Forming Limit Diagram of AA5083
    Zhalehfar, F.
    Hosseinipour, S. J.
    Nourouzi, S.
    Gorji, A. H.
    INTERNATIONAL CONFERENCE ON ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, PTS ONE AND TWO, 2010, 1315 : 353 - 358
  • [7] Constitutive modeling for the simulation of the Superplastic forming of AA5083
    Firas, Jarrar (fjarrar@pi.ac.ae), 1600, Trans Tech Publications Ltd (838-839):
  • [8] Experimental and theoretical investigation of strain path change effect on forming limit diagram of AA5083
    Farhad Zhalehfar
    Ramin Hashemi
    Seyed Jamal Hosseinipour
    The International Journal of Advanced Manufacturing Technology, 2015, 76 : 1343 - 1352
  • [9] Forming limit analysis of friction stir tailor welded AA5083 and AA7075 sheets in single point incremental forming
    Gautam Kumar
    Kuntal Maji
    International Journal of Material Forming, 2022, 15
  • [10] Forming limit analysis of friction stir tailor welded AA5083 and AA7075 sheets in single point incremental forming
    Kumar, Gautam
    Maji, Kuntal
    INTERNATIONAL JOURNAL OF MATERIAL FORMING, 2022, 15 (03)