Impact essential work of fracture; fracture toughness; polymer; polytetrafluoroethylene; filled-PTFE; Charpy test; scanning electron microscope; GLASS-FIBER; COMPOSITES;
D O I
10.1177/09673911211003392
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Polytetrafluoroethylene (PTFE) polymer has a wide range of applications in various industries. Therefore, for designers it is essential to know the strength properties of the material under dynamic loads. In this study, pure-PTFE, bronze and carbon filled-PTFE are tested under dynamic load. In addition, pure and carbon filled specimens were used to determine the temperature effect of PTFE. All tests were carried out in the Charpy impact device according to impact essential work of fracture method. At 23 degrees C, pure-PTFE showed the highest impact strengths, bronze filled-PTFE and carbon filled-PTFE showed lower respectively and it has been found that the carbon filler increases the fracture toughness approximately two times at high temperature (I 50 degrees C). On fracture surfaces phase transitions effects of PTFE and behavior of fillers used were investigated with Scanning Electron Microscope.
引用
收藏
页码:S335 / S343
页数:9
相关论文
共 19 条
[1]   Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: A review [J].
Barany, T. ;
Czigany, T. ;
Karger-Kocsis, J. .
PROGRESS IN POLYMER SCIENCE, 2010, 35 (10) :1257-1287
[2]   The role of crystalline phase on fracture and microstructure evolution of polytetrafluoroethylene (PTFE) [J].
Brown, EN ;
Dattelbaum, DM .
POLYMER, 2005, 46 (09) :3056-3068
[3]   The effect of crystallinity on the fracture of polytetrafluoroethylene (PTFE) [J].
Brown, Eric N. ;
Rae, Philip J. ;
Orler, E. Bruce ;
Gray, George T., III ;
Dattelbaum, Dana M. .
MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2006, 26 (08) :1338-1343
[4]  
Cho JW, 2001, J APPL POLYM SCI, V80, P484
[5]   The molecular conformations of polytetrafluoroethylene: forms II and IV [J].
Clark, ES .
POLYMER, 1999, 40 (16) :4659-4665
[6]   Performance properties and applications of polytetrafluoroethylene (PTFE)-a review [J].
Dhanumalayan, E. ;
Joshi, Girish M. .
ADVANCED COMPOSITES AND HYBRID MATERIALS, 2018, 1 (02) :247-268
[7]   CRYSTAL-STRUCTURE OF POLY(TETRAFLUOROETHYLENE) HOMOPOLYMERS AND COPOLYMERS IN THE HIGH-PRESSURE PHASE [J].
EBY, RK ;
CLARK, ES ;
FARMER, BL ;
PIERMARINI, GJ ;
BLOCK, S .
POLYMER, 1990, 31 (12) :2227-2237
[8]  
Hanford W., 1946, J AM CHEM SOC, V68, P2082, DOI [10.1021/ja01214a062, DOI 10.1021/JA01214A062]
[9]   FLUOROCARBON RESINS IN CORROSION PREVENTION [J].
HOMSY, CA .
INDUSTRIAL AND ENGINEERING CHEMISTRY, 1964, 56 (03) :20-&
[10]   Effect of glass fiber and maleated ethylene-propylene rubber content on the impact fracture parameters of nylon 6 [J].
Laura, DM ;
Keskkula, H ;
Barlow, JW ;
Paul, DR .
POLYMER, 2001, 42 (14) :6161-6172