Effects of Hydrofluoric Acid Concentration and Etching Time on the Bond Strength to Ceramic-coated Zirconia

被引:6
作者
Jin, Chunxiao [1 ]
Wang, Jingrong [1 ]
Huang, Yutian [1 ]
Yu, Ping [2 ]
Xiong, Yuhuan [1 ]
Yu, Haiyang [3 ]
Gao, Shanshan [1 ]
机构
[1] Sichuan Univ, West China Hosp Stomatol, Natl Clin Res Ctr Oral Dis, State Key Lab Oral Dis, Chengdu, Peoples R China
[2] Chengdu Second Peoples Hosp, Dept Stomatol, Chengdu, Peoples R China
[3] Sichuan Univ, West China Hosp Stomatol, Natl Clin Res Ctr Oral Dis, Dept Prosthodont,State Key Lab Oral Dis, Chengdu, Peoples R China
关键词
ceramic-coated zirconia; etching; shear bond strength; surface roughness; SURFACE TREATMENTS; LUTING CEMENTS; Y-TZP; ADHESION; GLAZE; LAYER;
D O I
10.3290/j.jad.b2838165
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the effects of different hydrofluoric acid (HF) concentrations and etching times on the surface topography, roughness, and resin bond strength to ceramic-coated zirconia (CC), and to compare them with the effects of alumina air-abrasion combined with 10-MDP (AA). Materials and Methods: AA and CC specimens were divided into 12 groups (N = 10). The CC groups were etched with HF at different concentrations (5% or 9.5%) for various durations (0 min, 1 min, 2 min, 3 min, 5 min or 10 min). The surface morphology was analyzed using SEM. Energy-dispersive x-ray spectroscopy (EDS) and x-ray diffraction (XRD) were performed for chemical and crystalline-phase analyses. Surface roughness (Ra) and shear bond strength (SBS) were recorded and statistically analyzed. Results: The SBS of CC groups initially increased, but then decreased with etching time for both HF acid concentrations. The 9.5% HF group displayed more marked topographical changes and higher Ra compared with the 5% HF group for the same etching period. Mean SBS was lower in the AA group compared with the CC groups etched with 5% HF for 2-10 min and 9.5% HF for 1-3 min (p < 0.05). Conclusions: Different HF concentrations and etching times influenced the surface topography, roughness, and resin bond strength of/to ceramic-coated zirconia. Etching with 5% HF for 5 min and with 9.5% HF for 2 min, respectively, provided the highest SBS.
引用
收藏
页码:125 / 135
页数:11
相关论文
共 50 条
  • [1] Effects of Different Primers on the Bond Strength to Properly and Excessively Etched Ceramic-coated Zirconia
    Deng, J.
    Jin, C.
    Zhu, L.
    Liu, L.
    Huang, Y.
    Zhao, P.
    Gao, S.
    OPERATIVE DENTISTRY, 2023, 48 (05) : 552 - 563
  • [2] Effect of Hydrofluoric Acid Concentration and Etching Time on Bond Strength to Lithium Disilicate Glass Ceramic
    Puppin-Rontani, J.
    Sundfeld, D.
    Costa, A. R.
    Correr, A. B.
    Puppin-Rontani, R. M.
    Borges, G. A.
    Sinhoreti, M. A. C.
    Correr-Sobrinho, L.
    OPERATIVE DENTISTRY, 2017, 42 (06) : 606 - 615
  • [3] Effect of etching with low concentration hydrofluoric acid on the bond strength of CAD/CAM resin block
    Niizuma, Yuiko
    Kobayashi, Mikihiro
    Toyama, Toshinari
    Manabe, Atsufumi
    DENTAL MATERIALS JOURNAL, 2020, 39 (06) : 1000 - 1008
  • [4] Effect of Low-Concentration Hydrofluoric Acid Etching on Shear Bond Strength and Biaxial Flexural Strength after Thermocycling
    Kang, You-Jung
    Shin, Yooseok
    Kim, Jee-Hwan
    MATERIALS, 2020, 13 (06)
  • [5] Hydrofluoric acid concentration, time and use of phosphoric acid on the bond strength of feldspathic ceramics
    Duarte Moura, Dayanne Monielle
    Medeiros de Araujo, Arthur Magno
    de Souza, Karina Barbosa
    Verissimo, Aretha Heitor
    Mendes Tribst, Joao Paulo
    de Assuncao e Souza, Rodrigo Othavio
    BRAZILIAN ORAL RESEARCH, 2020, 34
  • [6] Effect of hydrofluoric acid concentration and etching duration on select surface roughness parameters for zirconia
    Smielak, Beata
    Klimek, Leszek
    JOURNAL OF PROSTHETIC DENTISTRY, 2015, 113 (06) : 596 - 602
  • [7] Shear bond strength of zirconia ceramic to the primary tooth dentin
    Tuloglu, N.
    Akay, C. G.
    Bayrak, S.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2020, 23 (06) : 792 - 797
  • [8] Effect of 9% Hydrofluoric Acid Gel Hot-Etching Surface Treatment on Shear Bond Strength of Resin Cements to Zirconia Ceramics
    Kim, So-Hyun
    Cho, Sung-Chan
    Lee, Myung-Hyun
    Kim, Hyo-Jung
    Oh, Nam-Sik
    MEDICINA-LITHUANIA, 2022, 58 (10):
  • [9] Effect of femtosecond laser and silica coating on the bond strength of zirconia ceramic
    Zhou, Hongbo
    Yu, Chen
    Qi, Cheng
    Qiu, Dingxiang
    Zhang, Shusen
    Li, Jilin
    Hu, Youwang
    ADVANCES IN APPLIED CERAMICS, 2020, 119 (5-6) : 276 - 283
  • [10] Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: Effect of etching time and hydrofluoric acid concentration
    Monteiro, Jaiane Bandoli
    Oliani, Marcelo Gallo
    Guilardi, Luis Felipe
    Prochnow, Catina
    Rocha Pereira, Gabriel Kalil
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2018, 77 : 375 - 382