Preparation and characterization of spinel-type Mn Ni Co O negative temperature coefficient ceramic thermistors

被引:103
作者
De Vidales, JLM
Garcia-Chain, P
Rojas, RM
Vila, E
Garcia-Martinez, O
机构
[1] CSIC, Inst Ciencia Mat Madrid, E-28049 Madrid, Spain
[2] Autonomous Univ Madrid, Fac Ciencias C 6, E-28049 Madrid, Spain
[3] INYSA SA, Madrid 28108, Spain
关键词
D O I
10.1023/A:1004351809932
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Powders of ternary Mn-Ni-Co oxide negative temperature coefficient thermistors were synthesized by a low-temperature alternative route. The procedure allowed straightforward preparation without the addition of any binder, of highly densified Mn-Ni-Co-O semiconducting ceramics as cubic single-phase spinels, at relatively moderate temperature (approximate to 1000 degrees C). A tentative cation distribution for the Mn1.5Ni0.6Co0.9O4 spinel oxide has been proposed, and its variation with temperature has also been considered. The dilatometric and X-ray powder diffraction studies carried out for Mn1.5Ni0.6Co0.9O4 showed that sintering takes place in a single stage between 900 and 1000 degrees C, and yields highly densified ceramic with an apparant density larger than 96% of the calculated X-ray density. Scanning electron microscopy showed different microstructures for the Mn(1.5)Ni(0.6)Co(0.9)O(4)pinel oxide, depending on sintering conditions. The value of the sensitivity index, beta = 3068 K, indicates a good technological thermistor performance for this material. (C) 1998 Chapman & Hall.
引用
收藏
页码:1491 / 1496
页数:6
相关论文
共 17 条