Preparation of β-TCP/TiO2 composite by hot-pressing

被引:5
作者
Lee, Jong Kook [1 ]
Jung, Hang Chul [1 ]
Seo, Dong Seok [2 ]
Kim, Hwan [2 ]
Hwang, Kyu Hong [3 ]
机构
[1] Chosun Univ, Dept Adv Mat Engn, Kwangju 501759, South Korea
[2] Seoul Natl Univ, Sch Mat Sci & Engn, Seoul 151, South Korea
[3] Gyeongsang Natl Univ, Sch Mat Engn, Jinju 660701, South Korea
来源
NANOSCIENCE AND TECHNOLOGY, PTS 1 AND 2 | 2007年 / 121-123卷
关键词
hydroxyapatite; tricalcium phosphate; TiO2; dissolution; hardness; hot-pressing;
D O I
10.4028/www.scientific.net/SSP.121-123.983
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, tricalcium phosphate [TCP, beta-Ca-3(PO4)(2)]/titania composite were prepared with different ratio of 75/25, 50/50 and 25/75 (HA/TiO2, wt %). The TiO2 and hydroxyapatite (HA) powders, as starting materials, were synthesized by precipitation and hydrothermal methods, respectively. The sintered bodies of beta-TCP/TiO2 composite were prepared by hot pressing at pressure of 30 MPa and temperature of 800-1000 degrees C for 30 min under the pressure of 30 MPa in N-2 atmosphere. During the sintering process, hydroxyapatite was decomposed to beta-TCP and CaTiO3 at elevated temperature because TiO2 could accelerate the decomposition of hydroxyapatite. The hot-pressed composite with 98% of sintered density, showed high value of 1080 Hv in hardness, compared with the pure hydroxyapatite (600 Hv) before immersion in distilled water. Increasing sintering temperature led densification of the composite with moderately uniform microstructures. As increasing the amount of TiO2, the surface of the composite was less damaged or dissolved.
引用
收藏
页码:983 / 986
页数:4
相关论文
共 11 条
  • [1] PORES AND GRAIN GROWTH KINETICS
    BROOK, RJ
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1969, 52 (06) : 339 - &
  • [2] Hench LL, 1998, J AM CERAM SOC, V81, P1705
  • [3] IOKU K, 1991, J CERAM SOC JPN, V99, P191
  • [4] LACOUT JL, 1984, CR ACAD SCI II, V298, P173
  • [5] BONELIKE HYDROXYAPATITE INDUCTION BY A GEL-DERIVED TITANIA ON A TITANIUM SUBSTRATE
    LI, PJ
    KANGASNIEMI, I
    DEGROOT, K
    KOKUBO, T
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (05) : 1307 - 1312
  • [6] TENSILE-STRENGTH OF THE INTERFACE BETWEEN HYDROXYAPATITE AND BONE
    LIN, H
    XU, HC
    DEGROOT, K
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1992, 26 (01): : 7 - 18
  • [7] Sintering of zirconia coated hydroxyapatite particles
    Matsuno, T
    Watanabe, K
    Ono, K
    Koishi, M
    [J]. JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1996, 104 (10) : 945 - 948
  • [8] Preparation and characterisation of titania/hydroxyapatite composite coatings obtained by sol-gel process
    Milella, E
    Cosentino, F
    Licciulli, A
    Massaro, C
    [J]. BIOMATERIALS, 2001, 22 (11) : 1425 - 1431
  • [9] In vitro bioactivity of a biocomposite fabricated from HA and Ti powders by powder metallurgy method
    Ning, CQ
    Zhou, Y
    [J]. BIOMATERIALS, 2002, 23 (14) : 2909 - 2915
  • [10] Calcium phosphate apatites with variable Ca/P atomic ratio III. Mechanical properties and degradation in solution of hot pressed ceramics
    Raynaud, S
    Champion, E
    Lafon, JP
    Bernache-Assollant, D
    [J]. BIOMATERIALS, 2002, 23 (04) : 1081 - 1089