VHCF response of heat-treated SLM Ti6A14V Gaussian specimens with large loaded volume

被引:28
|
作者
Tridello, A. [1 ]
Fiocchi, J. [2 ]
Biffi, C. A. [2 ]
Chiandussi, G. [1 ]
Rossetto, M. [1 ]
Tuissi, A. [2 ]
Paolino, D. S. [1 ]
机构
[1] Politecn Torino, Dept Mech & Aerosp Engn, Corso Duca Abruzzi 24, I-10129 Turin, Italy
[2] CNR, Inst Condensed Matter Chem & Technol Energy, Unit Lecco, CNR ICMATE, Via G Previati 1E, I-23900 Lecce, Italy
来源
25TH INTERNATIONAL CONFERENCE ON FRACTURE AND STRUCTURAL INTEGRITY | 2019年 / 18卷
关键词
Additive Manufacturing (AM); Selective Laser Melting (SLM); Very High Cycle Fatigue (VHCF); Ti6A14V alloy; MANUFACTURED TI-6AL-4V; ALSI10MG SPECIMENS; STRENGTH; BEHAVIOR;
D O I
10.1016/j.prostr.2019.08.171
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Among the materials used for the production of components through Additive Manufacturing (AM) processes, the Selective -Laser-Melting (SLM) Ti6A14V alloy is widely employed in aerospace applications for its high specific strength and in biomedical applications for its good biocompatibility. Actual structural applications are generally limited to static loading conditions where the large defects originating during the SLM process do not play a significant role for the static failure. On the contrary, the same defects strongly affect the fatigue response of the parts since they act as crack initiation sites that rapidly lead to fatigue failure. In the literature, a lot of research has been carried out to investigate the quasi-static and the High-Cycle Fatigue properties of the SLM Ti6A14V alloy but there are still few studies on its Very -High-Cycle Fatigue (VHCF) response. In the paper, the VHCF response of Ti6A14V specimens, which are vertically orientated during the SLM building and then subjected to a conventional heat treatment (2 hours heating in vacuum at 850 C), is experimentally assessed. Ultrasonic VHCF tests are carried out on Gaussian specimens with a large risk-volume (2300 mm3). Fracture surfaces are investigated for revealing the defect originating the fatigue failure. The Stress Intensity Factor Threshold associated to the experimental failures is finally estimated. 2019 The Authors. Published by Elsevier B.V.
引用
收藏
页码:314 / 321
页数:8
相关论文
共 22 条
  • [21] Implementation of miniature tensile specimens in mechanical properties assessment of directed energy deposited Ti-6Al-4V: As-built and heat treated
    Alipour, Saeid
    Wu, Sung-Heng
    Liou, Frank
    Emdadi, Arezoo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 921
  • [22] Unique opportunities for microstructure engineering via trace B4C addition to Ti-6Al-4V through laser powder bed fusion process: As-built and heat-treated scenarios
    Fereiduni, Eskandar
    Ghasemi, Ali
    Elbestawi, Mohamed
    ADDITIVE MANUFACTURING, 2022, 50 : 1 - 21