The role of normal and activated bentonite on the pelletization of barite iron ore concentrate and the quality of pellets

被引:29
作者
Mohamed, OA
Shalabi, MEH
El-Hussiny, NA
Khedr, MH
Mostafa, F
机构
[1] CMRDI, Cairo, Egypt
[2] Cairo Univ, Fac Sci, Cairo, Egypt
关键词
pelletization; bentonite; iron ore concentrate; strength; reduction;
D O I
10.1016/S0032-5910(02)00205-X
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The essential parameters affecting the pelletization process of high barite iron ore concentrate were studied using the Egyptian normal and activated bentonite as binder materials. The metallurgical properties of green, dried and fired pellets were studied using chemical and X-ray analyses. The average strength of fired pellets 1.5% normal bentonite and fired 1300 degreesC for 25 min exceeded 200 kg/pellet. Using activated bentonite produced a lower kg/pellet value. Meanwhile, the productivity of green pellets decreased when the last binder was used. (C) 2002 Published by Elsevier Science B.V.
引用
收藏
页码:277 / 282
页数:6
相关论文
共 22 条
[1]  
ABOUZEID AZM, 1985, POWDER TECHNOL, P225
[2]  
AHMED YMZ, 1993, THESIS AIN SHAMS U
[3]  
[Anonymous], 1968, CLAY MINER
[4]  
Ball D.F., 1973, AGGLOMERATION IRON O
[5]  
BALL DF, 1960, T I MIN METALL C, V79, P189
[6]  
BALL DF, 1974, I MIN METALL, P47
[7]  
COOKE SRB, 1955, CHEM ENG PROG, P368
[8]  
DAVISION J, 1969, IND MINERAL, P27
[9]  
DOR A.A., 1970, 9 INT MIN PROC C PRA, VI, P173
[10]  
EKETORP S, 1962, STEEL MAK CHIPM C CA, P180