Nanostructured 2024Al-SiCp composite coatings

被引:9
|
作者
Tailor, S. [1 ,2 ]
Mohanty, R. M. [3 ]
Sharma, V. K. [1 ]
Soni, P. R. [1 ]
Doub, A. V. [2 ]
机构
[1] Malaviya Natl Inst Technol, Dept Met & Mat Engn, Jaipur 302017, Rajasthan, India
[2] Natl Univ Sci & Technol, NUST MISIS, Moscow, Russia
[3] CSIR, CSIR HQS, Rafi Marg, New Delhi 110001, India
关键词
2024 aluminium alloy; Metal matrix composites (MMCs); Mechanical alloying (MA); Adhesion; Wear; Plasma spray coatings; ALUMINUM-MATRIX COMPOSITES; SLIDING WEAR BEHAVIOR; MECHANICAL-PROPERTIES; TRIBOLOGICAL BEHAVIOR; NANOCRYSTALLINE AL; RESIDUAL-STRESSES; GRAIN-SIZE; FRICTION; PARTICLES; SURFACE;
D O I
10.1179/1743294414Y.0000000391
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microstructure and mechanical properties of plasma sprayed nanostructured 2024Al alloy were investigated before and after adding SiC particles on weathering steel (Cor-Ten A242) substrate. Mechanical alloying (MA) was used to synthesise the nanostructured 2024Al and 2024Al-15 wt-% SiC composite powders. X-ray diffraction studies showed SiCp embedment in the Al matrix after MA and nanograins in the MA powder and coatings. It was found that the porosity level in the coating was reduced to 2% and the coating hardness was increased to 3276 MPa. The high adhesion strength of the coatings observed can be attributed to the higher degree of diffusion at the interface. In these experiments, there was 60% decrease in the wear rate of the coatings. Results show that MA decreases the size of the matrix grains to 45 nm for the MA powder and 17 nm for the coating. The results of mechanical and wear tests also indicate that MA and the addition of SiC particles increased the strength, hardness and wear resistance of 2024Al and remarkably decreased its ductility.
引用
收藏
页码:526 / 534
页数:9
相关论文
共 50 条
  • [1] Wear Behavior of Plasma Sprayed Nanostructured Al-SiCp Composite Coatings: A Comparative Study
    Tailor, Satish
    Mohanty, R. M.
    Soni, P. R.
    Doub, A. V.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (06) : 1179 - 1191
  • [2] Friction stir welding of SiCp/Al composite and 2024 Al alloy
    Xiao, B. L.
    Wang, D.
    Bi, J.
    Zhang, Z.
    Ma, Z. Y.
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 1500 - 1505
  • [3] Investigation of friction and wear behaviors of 2024 Al and 2024 Al/SiCp composite at elevated temperatures
    Abarghouie, S. M. R. Mousavi
    Reihani, S. M. Seyed
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 501 (02) : 326 - 332
  • [4] Aging behavior of a 2024 Al alloy-SiCp composite
    Abarghouie, S. M. R. Mousavi
    Reihani, S. M. Seyed
    MATERIALS & DESIGN, 2010, 31 (05) : 2368 - 2374
  • [5] Compressive and wear behaviors of bulk nanostructured Al2024 alloy
    Jafari, M.
    Enayati, M. H.
    Abbasi, M. H.
    Karimzadeh, F.
    MATERIALS & DESIGN, 2010, 31 (02) : 663 - 669
  • [6] Tribology of SiCp reinforced Al-12Si matrix composite coatings in water
    Paksoy, Ahmet Hilmi
    Deprem, Ozde
    Tazegul, Onur
    Cimenoglu, Huseyin
    TRIBOLOGY INTERNATIONAL, 2017, 110 : 392 - 400
  • [7] Effects of solid solution treatment on microstructure and mechanical properties of SiCp/2024 Al composite: A comparison with 2024 Al alloy
    Liu, G. F.
    Chen, T. J.
    Wang, Z. J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 817
  • [8] Properties and microstructure of Al-11Si/SiCp composite coatings fabricated by thermal spray
    Torres, B.
    Campo, M.
    Rams, J.
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (14) : 1947 - 1955
  • [9] Laser welding of SiCp/2024Al composites with novel TiB2/2024Al composite filler
    Han, Ke
    Han, Rui
    Li, Xiaopeng
    Zhang, Xingyue
    Li, Hongliang
    Wang, Jianhao
    Wang, Kehong
    MATERIALS LETTERS, 2023, 349
  • [10] Experimental and modeling investigation on SiCp distribution in powder metallurgy processed SiCp/2024 Al composites
    Liu, Z. Y.
    Wang, Q. Z.
    Xiao, B. L.
    Ma, Z. Y.
    Liu, Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (21-22): : 5582 - 5591