共 32 条
- [1] Early Steps of Pore Formation During Stainless Steel Oxides Reduction with Hydrogen at 1373 K (1100 °C) [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2016, 47 (02): : 1445 - 1452
- [3] Mechanism of Iron Oxide Scale Reduction in 5%H2-N2 Gas at 650-900 °C [J]. OXIDATION OF METALS, 2017, 88 (5-6): : 687 - 717
- [4] Longer Term Oxidation Kinetics of Low Carbon, Low Silicon Steel in 17H2O-N2 at 900°C [J]. OXIDATION OF METALS, 2016, 85 (5-6): : 489 - 507
- [5] A study of the scale structure of hot-rolled steel strip by simulated coiling and cooling [J]. OXIDATION OF METALS, 2000, 53 (5-6): : 539 - 560
- [10] High-Temperature Oxidation and Pickling Behaviour of HSLA Steels [J]. OXIDATION OF METALS, 2018, 89 (1-2): : 33 - 48