W-25%Re-HfC composite materials for Pin tool material applications: Synthesis and consolidation

被引:25
作者
Iqbal, Zafar [1 ]
Saheb, Nouari [1 ,2 ]
Shuaib, Abdel Rahman [1 ]
机构
[1] King Fahd Univ Petr & Minerals, Dept Mech Engn, Dhahran 31261, Saudi Arabia
[2] King Fahd Univ Petr & Minerals, Ctr Res Excellence Nanotechnol, Dhahran 31261, Saudi Arabia
关键词
Mechanical alloying; Spark plasma sintering; Hard metals; Composites; Microstructure; Density; Hardness; METAL-MATRIX COMPOSITES; AL-SIC NANOCOMPOSITES; MECHANICAL-PROPERTIES; NITRIDE CERAMICS; BEHAVIOR; TUNGSTEN; ALLOYS; DENSIFICATION; EVOLUTION; GROWTH;
D O I
10.1016/j.jallcom.2016.03.030
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The development of tool materials for high temperature applications such as friction stir welding of steels and high strength materials remain a key challenge because these materials are difficult to synthesize and consolidate by conventional means. In this work, nanostructured W-25 wt.%Re alloy and W-25Re-HfC composites of uniform microstructure containing 5 and 10 vol.% of HfC particles, were developed by mechanical alloying (MA) and spark plasma sintering (SPS) techniques. The effect of processing parameters and reinforcement content on the microstructure, densification, and properties of the developed materials was investigated. Mechanical alloying of the as-received and partially alloyed W-25 wt.%Re powder for 25 h yielded a single nanostructured solid solution with a crystallite size of 13 nm and increased its lattice strain to 0.75%. The fully alloyed powder was reinforced with 5 and 10 vol.% of HfC particles and further milled for 15 h, this led to the formation of composite powders with a uniform distribution of particles in the matrix. The uniform distribution of HfC particles, obtained by mechanical alloying, was maintained in the consolidated samples. Crystallite size of the matrix phase in the sintered composites remained in the nanometer range and did not exceed 100 nm. Partially and fully alloyed monolithic W-25 wt.%Re alloys, spark plasma sintered at 1800 degrees C for 10 min, had relative density values of 98.2 and 97.8%, respectively. W-25Re-HfC composites containing 5 and 10 vol.% HfC, spark plasma sintered at 1800 degrees C for 10 min, had relative density values of 96.9 and 96.2%, respectively. The composite containing 10 vol.% of HfC possessed the highest Vickers hardness value of 495. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:189 / 199
页数:11
相关论文
共 51 条
  • [1] Porosity influence on the mechanical properties of polycrystalline zirconium nitride ceramics
    Adachi, Jun
    Kurosaki, Ken
    Uno, Masayoshi
    Yamanaka, Shinsuke
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2006, 358 (2-3) : 106 - 110
  • [2] Microstructure and compressibility of SiC nanoparticles reinforced Cu nanocomposite powders processed by high energy mechanical milling
    Akbarpour, M. R.
    Salahi, E.
    Hesari, F. Alikhani
    Simchi, A.
    Kim, H. S.
    [J]. CERAMICS INTERNATIONAL, 2014, 40 (01) : 951 - 960
  • [3] THE STRUCTURE OF AMORPHOUS AND NANOCRYSTALLINE W-FE ALLOYS PREPARED BY HIGH-ENERGY BALL MILLING
    BOLDRICK, MS
    YANG, E
    WAGNER, CNJ
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 1992, 150 (1-3) : 478 - 482
  • [4] Buffa Gianluca, 2012, P NAMRI SME, V40
  • [5] Candido G.M., 2012, Materials Science Forum, V660-661, P317
  • [6] Metal Matrix Composites Reinforced by Nano-Particles-A Review
    Casati, Riccardo
    Vedani, Maurizio
    [J]. METALS, 2014, 4 (01) : 65 - 83
  • [7] Chawla N, 2001, ADV ENG MATER, V3, P357, DOI 10.1002/1527-2648(200106)3:6<357::AID-ADEM357>3.0.CO
  • [8] 2-I
  • [9] A strain gradient-strengthening law for particle reinforced metal matrix composites
    Dai, LH
    Ling, Z
    Bai, YL
    [J]. SCRIPTA MATERIALIA, 1999, 41 (03) : 245 - 251
  • [10] Dawes C., 1995, TWI Bulletin, V6, P124