Elucidating Copper Dissolution Phenomenon in Li-Ion Cells under Overdischarge Extremes

被引:99
作者
Fear, Conner [1 ]
Juarez-Robles, Daniel [1 ]
Jeevarajan, Judith A. [2 ]
Mukherjee, Partha P. [1 ]
机构
[1] Purdue Univ, Sch Mech Engn, W Lafayette, IN 47907 USA
[2] Underwriters Labs Inc, Electrochem Safety, Northbrook, IL 60062 USA
关键词
DISCHARGE CONDITIONS; THERMAL-STABILITY; OVER-DISCHARGE; BATTERIES; PERFORMANCE; OVERCHARGE; PROTECTION;
D O I
10.1149/2.0671809jes
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The mechanisms driving the thermo-electrochemical response of commercial lithium-ion cells under extreme overdischarge conditions (< 0.0 V) are investigated in the context of copper dissolution from the anodic current collector. A constant current discharge with no lower cutoff voltage was used to emulate the effects of forced overdischarge, as commonly experienced by serially connected cells in an unbalanced module. Cells were overdischarged to 200% DOD (depth of discharge) at C/10 and 1C rates to develop an understanding of the overdischarge extremes. Copper dissolution began when a cell reached its minimum voltage level (between -1.3 V and -1.5 V), where the anode potential reached a maximum value of similar to 4.8 V vs. Li/Li+. Deposition of copper on the cathode, anode, and separator surfaces was observed in all overdischarged cells, verified with EDS/SEM results, which further suggests the formation of internal shorts, although the cell failures proved to be relatively benign. The maximum cell surface temperature during overdischarge was found to be highly rate-dependent, with the 1C-rate cell experiencing temperatures as high as 79 degrees C. Concentration polarization and solid electrolyte interphase (SEI) layer breakdown prior to the initiation of copper dissolution are proposed to be the main sources of heat generation during overdischarge. (C) The Author(s) 2018. Published by ECS.
引用
收藏
页码:A1639 / A1647
页数:9
相关论文
共 25 条
  • [1] [Anonymous], US TODAY
  • [2] Chanson C., 2013, Safety of Lithium-Ion Batteries, P10
  • [3] Chemical overcharge and overdischarge protection for lithium-ion batteries
    Chen, J
    Buhrmester, C
    Dahn, JR
    [J]. ELECTROCHEMICAL AND SOLID STATE LETTERS, 2005, 8 (01) : A59 - A62
  • [4] Enhancement of thermal stability and cycling performance in lithium-ion cells through the use of ceramic-coated separators
    Choi, Ji-Ae
    Kim, Sa Heum
    Kim, Dong-Won
    [J]. JOURNAL OF POWER SOURCES, 2010, 195 (18) : 6192 - 6196
  • [5] Challenges in the development of advanced Li-ion batteries: a review
    Etacheri, Vinodkumar
    Marom, Rotem
    Elazari, Ran
    Salitra, Gregory
    Aurbach, Doron
    [J]. ENERGY & ENVIRONMENTAL SCIENCE, 2011, 4 (09) : 3243 - 3262
  • [6] Investigating lithium-ion battery materials during overcharge-induced thermal runaway: an operando and multi-scale X-ray CT study
    Finegan, Donal P.
    Scheel, Mario
    Robinson, James B.
    Tjaden, Bernhard
    Di Michiel, Marco
    Hinds, Gareth
    Brett, Dan J. L.
    Shearing, Paul R.
    [J]. PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2016, 18 (45) : 30912 - 30919
  • [7] Island growth in electrodeposition
    Guo, Lian
    Oskam, Gerko
    Radisic, Aleksandar
    Hoffmann, Peter M.
    Searson, Peter C.
    [J]. JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2011, 44 (44)
  • [8] Guo R., 2016, SCI REPORTS
  • [9] Failure Investigation of LiFePO4 Cells in Over-Discharge Conditions
    He, Hao
    Liu, Yadong
    Liu, Qi
    Li, Zhefei
    Xu, Fan
    Dun, Clif
    Ren, Yang
    Wang, Mei-xian
    Xie, Jian
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2013, 160 (06) : A793 - A804