Flame retardancy of microcellular poly(lactic acid) foams prepared by supercritical CO2-assisted extrusion

被引:30
作者
Vadas, Daniel [1 ]
Igricz, Tamas [1 ]
Sarazin, Johan [2 ]
Bourbigot, Serge [2 ]
Marosi, Gyorgy [1 ]
Bocz, Katalin [1 ]
机构
[1] Budapest Univ Technol & Econ, Dept Organ Chem & Technol, Fac Chem Technol & Biotechnol, Muegyet Rkp 3, H-1111 Budapest, Hungary
[2] Univ Lille, Unite Mat & Transformat, UMR CNRS 8207, ENSCL, Ave Mendeleiev CS 90108, F-59652 Villeneuve Dascq, France
基金
匈牙利科学研究基金会;
关键词
Poly(lactic acid); Extrusion foaming; Flame retardancy; Intumescence; Cellulose; THERMAL-PROPERTIES; COMPOSITES; POLYLACTIDE; FLAMMABILITY; CO2; MONTMORILLONITE; CRYSTALLIZATION; CRYSTALLINITY; DECOMPOSITION; STABILITY;
D O I
10.1016/j.polymdegradstab.2018.04.021
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Flame-retardant-treated cellulose (FR-cell) was used as bio-based charring agent in combination with ammonium polyphosphate (APP) based intumescent flame retardant (IFR) system to reduce the flammability of poly(lactic acid) (PLA) foams produced by supercritical carbon dioxide (sc-CO2) assisted extrusion. FR-cell was obtained by surface treatment of cellulose with diammonium phosphate (DAP) and boric acid (BA). To enhance foamability, the inherently low melt strength and slow crystallization rate of PLA was increased by adding epoxy-based chain extender (CE) and montmorillonite (MMT) nanoclay, respectively. The morphology of the foams was examined using water displacement method, scanning electron microscopy (SEM) and energy dispersive X-ray spectrometry (EDS). Thermal properties were assessed using differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). Flammability was evaluated by limiting oxygen index (LOI) measurements, UL-94 tests and pyrolysis combustion flow calorimetry (PCFC). The continuous extrusion foaming technique allowed the preparation of low density PLA foams with uniform microcellular structure and void fractions higher than 90% accompanied with increased crystallinity of up to 19%. Despite the high expansion ratios (i.e. high surface area), the PLA foams showed excellent flame retardancy, UL-94V-0 rate and LOI value of 31.5 vol% was achieved with an additive content as small as 19.5%. However, the flame retardant synergism evinced between IFR and MMT proved to be less pronounced in the expanded foams compared to bulk materials with identical additive contents. (C) 2018 Elsevier Ltd. All rights reserved.
引用
收藏
页码:100 / 108
页数:9
相关论文
共 34 条
[1]  
[Anonymous], 2014, CLARIANT PRODUCTS EX
[2]   Crystallization kinetics of poly(lactic acid)-talc composites [J].
Battegazzore, D. ;
Bocchini, S. ;
Frache, A. .
EXPRESS POLYMER LETTERS, 2011, 5 (10) :849-858
[3]   Characterisation of natural fibre reinforced PLA foams prepared by supercritical CO2 assisted extrusion [J].
Bocz, K. ;
Tabi, T. ;
Vadas, D. ;
Sauceau, M. ;
Fages, J. ;
Marosi, Gy. .
EXPRESS POLYMER LETTERS, 2016, 10 (09) :771-779
[4]   Flame retarded self-reinforced poly(lactic acid) composites of outstanding impact resistance [J].
Bocz, Katalin ;
Domonkos, Martina ;
Igricz, Tamas ;
Kmetty, Akos ;
Barany, Tamas ;
Marosi, Gyorgy .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 70 :27-34
[5]   Flax fibre reinforced PLA/TPS biocomposites flame retarded with multifunctional additive system [J].
Bocz, Katalin ;
Szolnoki, Beata ;
Marosi, Attila ;
Tabi, Tamas ;
Wladyka-Przybylak, Maria ;
Marosi, Gyoergy .
POLYMER DEGRADATION AND STABILITY, 2014, 106 :63-73
[6]  
Bocz K, 2013, POLIMERY-W, V58, P385
[7]   Determination of kinetics and thermodynamics of thermal decomposition for polymers containing reactive flame retardants: Application to poly(lactic acid) blended with melamine and ammonium polyphosphate [J].
Ding, Yan ;
McKinnon, Mark B. ;
Stoliarov, Stanislav I. ;
Fontaine, Gaelle ;
Bourbigot, Serge .
POLYMER DEGRADATION AND STABILITY, 2016, 129 :347-362
[8]   Flame retardant properties and mechanism of an efficient intumescent flame retardant PLA composites [J].
Feng, Caimin ;
Liang, Minyi ;
Jiang, Jiali ;
Huang, Jianguang ;
Liu, Hongbo .
POLYMERS FOR ADVANCED TECHNOLOGIES, 2016, 27 (05) :693-700
[9]   INVESTIGATION OF STRUCTURE OF SOLUTION GROWN CRYSTALS OF LACTIDE COPOLYMERS BY MEANS OF CHEMICAL-REACTIONS [J].
FISCHER, EW ;
STERZEL, HJ ;
WEGNER, G .
KOLLOID-ZEITSCHRIFT AND ZEITSCHRIFT FUR POLYMERE, 1973, 251 (11) :980-990
[10]   Intumescent Polylactide: A Nonflammable Material [J].
Fontaine, Gaelle ;
Bourbigot, Serge .
JOURNAL OF APPLIED POLYMER SCIENCE, 2009, 113 (06) :3860-3865