High Impact Properties of Polyketone/Polyamide-6 Alloys Induced by Characteristic Morphology and Water Absorption

被引:28
作者
Asano, Atsushi [2 ]
Nishioka, Maiko [1 ]
Takahashi, Yohei [1 ]
Kato, Atsushi [1 ]
Hikasa, Shigeki [3 ]
Iwabuki, Hitoshi [3 ]
Nagata, Kazuya [4 ]
Sato, Hidenori [1 ]
Hasegawa, Toshinori [1 ]
Sawabe, Hisahiro [1 ]
Arao, Masazumi [1 ]
Suda, Toshiya [1 ]
Isoda, Ayano [1 ]
Mukai, Mitsuo [1 ]
Ishikawa, Daisuke [1 ]
Izumi, Toshihiro [1 ]
机构
[1] NISSAN ARC LTD, Yokosuka, Kanagawa 2370061, Japan
[2] Natl Def Acad, Dept Appl Chem, Yokosuka, Kanagawa 2398686, Japan
[3] Ind Technol Ctr, Okayama 7011296, Japan
[4] Asahi Kasei Chem Corp, Adv Technol Dev Dept, Lab Plast, Kawasaki, Kanagawa 2100863, Japan
关键词
AMPLITUDE CROSS-POLARIZATION; NYLON-6 CLAY NANOCOMPOSITES; SOLID-STATE C-13; CRYSTALLINE-STRUCTURE; NMR; DEFORMATION; RELAXATION; DISPERSION; TOUGHNESS; STABILITY;
D O I
10.1021/ma901428z
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Nagata et al. recently developed high-impact polyketone/polyamide-6 (PK/PA) alloys and investigated their mechanical properties (Nagata et al, Polym. Prep. Jpn. 2006, 55, 4286-4287). This paper presents the results of investigations of their morphology, Such as the domain size of PA and PK, features of crystalline phase of PK (the long period and thickness of lamellae are deduced), and the change in crystalline form of PA in the PK/PA alloys, using solid-state nuclear magnetic resonance (NMR), small-angle X-ray scattering (SAXS), and transmission electron microscopy (TEM). Solid-state C-13 and N-15 NMR results revealed that the gamma crystalline phase of PA changes into it thermodynamically stable a crystalline phase after alloying with PK. The difference in the long period of lamellae of PK/PA alloys between dry and wet conditions is discussed. We conclude that the characteristic morphology of PK and humidity of the amorphous phase of PA in the wet condition are very important factors enabling the PK/PA alloys to exhibit high impact resistance, high-strength, and high modulus.
引用
收藏
页码:9506 / 9514
页数:9
相关论文
共 36 条
[1]  
Andreis M, 1995, ADV POLYM SCI, V124, P191
[2]   C-13 CP/MAS NMR-STUDY ON THE MISCIBILITY AND PHASE-SEPARATION OF A POLYSTYRENE POLY(VINYL METHYL-ETHER) BLEND [J].
ASANO, A ;
TAKEGOSHI, K ;
HIKICHI, K .
POLYMER, 1994, 35 (26) :5630-5636
[3]  
Asano A, 1998, STUD PHYS THEO CHEM, V84, P351, DOI 10.1016/S0167-6881(98)80018-9
[4]  
Asano A., 2008, POLYM PREPR, V49, P682
[5]  
Asano A., 2006, MODERN MAGNETIC RE 1, P627
[6]   Dynamics of polymer blends and NMR relaxation in solids [J].
Asano, Atsushi .
KOBUNSHI RONBUNSHU, 2007, 64 (07) :406-418
[7]   Melting Point and Domain Size of PVIBE/ε-PL/Saponite Clay Investigated by Solid-State 13C NMR [J].
Asano, Atsushi ;
Tanaka, Chikako ;
Kurotsu, Takuzo .
MACROMOLECULES, 2008, 41 (23) :9469-9473
[8]   HETERONUCLEAR DECOUPLING IN ROTATING SOLIDS [J].
BENNETT, AE ;
RIENSTRA, CM ;
AUGER, M ;
LAKSHMI, KV ;
GRIFFIN, RG .
JOURNAL OF CHEMICAL PHYSICS, 1995, 103 (16) :6951-6958
[9]  
BUCKNALL CB, 2000, POLYM BLENDS FORMULA, V2, pCH21
[10]  
Chen HB, 2000, J APPL POLYM SCI, V77, P928, DOI 10.1002/(SICI)1097-4628(20000725)77:4<928::AID-APP29>3.0.CO