Hot deformation behavior and microstructure evolution of a Mg-Gd-Nd-Y-Zn alloy

被引:15
作者
Hou, Xiu-Li [1 ]
Li, Yan [1 ]
Lv, Peng [1 ]
Cai, Jie [1 ]
Ji, Le [1 ]
Guan, Qing-Feng [1 ]
机构
[1] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212013, Peoples R China
基金
中国博士后科学基金;
关键词
Mg-Gd-Nd-Y-Zn alloy; Hot deformation; Microstructure; Dynamic recrystallization; MAGNESIUM ALLOY; TEXTURE; RECRYSTALLIZATION; PRECIPITATION; COMPRESSION; ALUMINUM;
D O I
10.1007/s12598-015-0507-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The hot deformation behavior of homogenized Mg-6.5Gd-1.3Nd-0.7Y-0.3Zn alloy was investigated during compression at temperatures of 250-400 degrees C and at strain rates ranging from 0.001 to 0.100 s(-1). Microstructure analyses show that the flow behaviors are associated with the deformation mechanisms. At the lower temperatures (250-300 degrees C), deformation twinning is triggered due to the difficult activation of dislocation cross-slip. Dynamic recrystallization (DRX) accompanied by dynamic precipitation occurs at the temperature of 350 degrees C and influences the softening behavior of the flow. DRX that develops extensively at original grain boundaries is the main softening mechanism at the high temperature of 400 degrees C and eventually brings a more homogeneous microstructure than that in other deformation conditions. The volume fraction of the DRXed grains increases with temperature increasing and decreases with strain rate increasing.
引用
收藏
页码:532 / 536
页数:5
相关论文
共 17 条
[1]   Effect of twinning on the deformation behavior of an extruded Mg-Zn-Zr alloy during hot compression testing [J].
Ai, W. -J. ;
Fang, G. ;
Zhou, J. ;
Leeflang, M. A. ;
Duszczyk, J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 :373-381
[2]   Hot working mechanisms and texture development in Mg-3Sn-2Ca-0.4Al alloy [J].
Dharmendra, C. ;
Rao, K. P. ;
Prasad, Y. V. R. K. ;
Hort, N. ;
Kainer, K. U. .
MATERIALS CHEMISTRY AND PHYSICS, 2012, 136 (2-3) :1081-1091
[3]   Effect of initial microstructure on ultrafine grain formation through warm deformation in medium-carbon steels [J].
Hase, Kazukuni ;
Tsuji, Nobuhiro .
SCRIPTA MATERIALIA, 2011, 65 (05) :404-407
[4]   Precipitation in a Mg-10Gd-3Y-0.4Zr (wt.%) alloy during isothermal ageing at 250°C [J].
He, S. M. ;
Zeng, X. Q. ;
Peng, L. M. ;
Gao, X. ;
Nie, J. F. ;
Ding, W. J. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2006, 421 (1-2) :309-313
[5]   Superior light metals by texture engineering: Optimized aluminum and magnesium alloys for automotive applications [J].
Hirsch, J. ;
Al-Samman, T. .
ACTA MATERIALIA, 2013, 61 (03) :818-843
[6]   Fabrication of extraordinary high-strength magnesium alloy by hot extrusion [J].
Homma, T. ;
Kunito, N. ;
Kamado, S. .
SCRIPTA MATERIALIA, 2009, 61 (06) :644-647
[7]   Structure and mechanical properties of extruded Mg-Gd based alloy sheet [J].
Hou, Xiuli ;
Peng, Qiuming ;
Cao, Zhanyi ;
Xu, Shiwei ;
Kamado, Shigeharu ;
Wang, Lidong ;
Wu, Yaoming ;
Wang, Limin .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 520 (1-2) :162-167
[8]  
Humphreys FJ, 2004, RECRYSTALLIZATION RE, V415
[9]  
Kainer K.U., 2003, MAGNESIUM ALLOYS TEC
[10]   Twinning, dynamic recovery and recrystallization in hot worked Mg-Al-Zn alloy [J].
Myshlyaev, MM ;
McQueen, HJ ;
Mwembela, A ;
Konopleva, E .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 337 (1-2) :121-133