Experimental investigation on fragmentation initiation of mm-sized coal particles in a drop-tube furnace

被引:11
作者
Zhong, Shan [1 ,2 ]
Baitalow, Felix [2 ]
Meyer, Bernd [2 ]
机构
[1] Sichuan Univ, Sch Chem Engn, Chengdu 610065, Sichuan, Peoples R China
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, Fuchsmuhlenweg 9, D-09599 Freiberg, Germany
关键词
Coal particle; Fragmentation initiation; Tensile stress; Porosity; Fragmentation resistance number; FLUIDIZED-BED COMBUSTION; THERMAL-STRESS; HEATING RATE; DEVOLATILIZATION; BEHAVIOR; PYROLYSIS; EVOLUTION; GASIFIER; FRACTURE; REACTOR;
D O I
10.1016/j.fuel.2018.06.059
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The investigation of mm-sized coal particle fragmentation initiation is of practical interest because of its great importance in the analysis of coal utilization processes such as combustion or gasification in fluidized-bed reactors. Fragmentation experiments were conducted within a drop-tube furnace with eleven kinds of coals of different sizes, and the influences of different factors were discussed. The fragmentation index increased monotonically as the temperature and particle size increase, and the heating rate at different conditions was estimated. No significant correlation was revealed between the fragmentation and the volatile matter, and the thermal stress was deemed to be the main cause of fragmentation. The influences of porosity and tensile strength on fragmentation were more pronounced. Generally, the fragmentation tended to be less extensive as the porosity and tensile strength increased. Accordingly, a parameter consisting of porosity and tensile strength was proposed and defined as the fragmentation resistance number (FRN). The results showed that the larger the FRN is, the more difficult the particles are to fragment; furthermore, the FRN was found to apply well for predicting the fragmentation initiation temperature (FIT) and evaluating fragmentation.
引用
收藏
页码:473 / 481
页数:9
相关论文
共 30 条
  • [1] MATHEMATICAL-MODELING OF DEVOLATILIZATION OF LARGE COAL PARTICLES IN A CONVECTIVE ENVIRONMENT
    ADESANYA, BA
    PHAM, HN
    [J]. FUEL, 1995, 74 (06) : 896 - 902
  • [2] CHAR FRAGMENTATION AND FLY-ASH FORMATION DURING PULVERIZED-COAL COMBUSTION
    BAXTER, LL
    [J]. COMBUSTION AND FLAME, 1992, 90 (02) : 174 - 184
  • [3] PRIMARY FRAGMENTATION IN FLUIDIZED-BED COMBUSTION OF ANTHRACITES
    CHIRONE, R
    MASSIMILLA, L
    [J]. POWDER TECHNOLOGY, 1991, 64 (03) : 249 - 258
  • [4] Chirone R., 1988, 22 S COMBUST COMBUST, V22, P267, DOI DOI 10.1016/S0082-0784(89)80033-5
  • [5] EFFECT OF POROSITY ON THERMAL STRESS FRACTURE
    COBLE, RL
    KINGERY, WD
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1955, 38 (01) : 33 - 37
  • [6] Experimental study on fragmental behavior of coals and biomasses during rapid pyrolysis
    Cui, Tongmin
    Xu, Jianliang
    Fan, Wenke
    Chang, Qinghua
    Yu, Guangsuo
    Wang, Fuchen
    [J]. BIORESOURCE TECHNOLOGY, 2016, 222 : 439 - 447
  • [7] Combustion-induced fragmentation behavior of isolated coal particles
    Dacombe, P
    Pourkashanian, M
    Williams, A
    Yap, L
    [J]. FUEL, 1999, 78 (15) : 1847 - 1857
  • [8] FRAGMENTATION AND SWELLING OF VARIOUS COALS DURING DEVOLATILIZATION IN A FLUIDIZED-BED
    DAKIC, D
    VANDERHONING, G
    VALK, M
    [J]. FUEL, 1989, 68 (07) : 911 - 916
  • [9] Evans I., 1966, The strength, fracture and workability of coal: a monograph on basic work on coal winning carried out by the Mining Research Establishment, V1st
  • [10] Weibull modulus and fracture strength of highly porous hydroxyapatite
    Fan, X.
    Case, E. D.
    Gheorghita, I.
    Baumann, M. J.
    [J]. JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2013, 20 : 283 - 295