Characterization of Fretting Fatigue Behavior of TiN/Ti Coating on Ti-811 Alloy at Increased Temperature

被引:1
作者
Zhang, Xiaohua [1 ]
Pan, Feng [1 ]
Xiang, Dinggen [1 ]
机构
[1] Northwestern Polytech Univ, Corros & Protect Res Lab, Xian 710072, Peoples R China
来源
PROCEEDINGS OF THE FIRST SYMPOSIUM ON AVIATION MAINTENANCE AND MANAGEMENT-VOL II | 2014年 / 297卷
关键词
Titanium alloy; Fretting fatigue; Ion-assisted deposition; Increased temperature; ENGINE;
D O I
10.1007/978-3-642-54233-6_77
中图分类号
V [航空、航天];
学科分类号
08 ; 0825 ;
摘要
A TiN/Ti composite coating has been prepared on a Ti-811 titanium alloy substrate by an ion-assisted arc deposition (IAAD) technique. The composition distribution, microhardness, ductility, tribological properties, and fretting fatigue resistance (FFR) at increased temperature of the coating have been investigated. The results indicate that the IAAD technique can be used to prepare a TiN/Ti composite coating with high hardness, good ductility, excellent bonding strength, and high load-bearing capability. The TiN/Ti composite coating can improve the resistance to wear and fretting fatigue (FF) of the Ti alloy at 350 degrees C because of the good toughness and high bonding strength of the IAAD TiN/Ti composite coating with excellent lubrication of Ti particles in the coating.
引用
收藏
页码:699 / 705
页数:7
相关论文
共 8 条
[1]   Fatigue fracture of crankshaft of an aircraft engine [J].
Bhaumik, SK ;
Rangaraju, R ;
Venkataswamy, MA ;
Bhaskaran, TA ;
Parameswara, MA .
ENGINEERING FAILURE ANALYSIS, 2002, 9 (03) :255-263
[2]   Effect of various surface conditions on fretting fatigue behavior of Ti-6Al-4V [J].
Hutson, AL ;
Niinomi, M ;
Nicholas, T ;
Eylon, D .
INTERNATIONAL JOURNAL OF FATIGUE, 2002, 24 (12) :1223-1234
[3]  
James C W, 2003, Acta Materialia, V51, P5775
[4]   Investigation into effects of re-shot-peening on fretting fatigue behavior of Ti-6Al-4V [J].
Lee, H ;
Mall, S ;
Sathish, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 390 (1-2) :227-232
[5]  
[刘道新 Liu Daoxin], 2005, [摩擦学学报, Tribology], V25, P13
[6]   Failure of connecting pins of a compressor disc in an aero engine [J].
Ray, AK ;
Das, G ;
Ranganath, VR ;
Goswami, B ;
Ghosh, RN .
ENGINEERING FAILURE ANALYSIS, 2004, 11 (04) :613-617
[7]   Fretting damage of TiN coated zircaloy-4 tube [J].
Sung, JH ;
Kim, TH ;
Kim, SS .
WEAR, 2001, 250 (250-251) :658-664
[8]  
Wei R, 2004, SURF COAT TECH, V192, P177