Fracture toughness of boride formed on low-alloy steels

被引:91
作者
Ucisik, AH
Bindal, C [1 ]
机构
[1] Sakarya Univ, Fac Engn, Dept Met Engn, TR-54040 Esentepe, Adapazari, Turkey
[2] Bogazici Univ, Inst Biomed Engn, TR-80815 Bebek, Istanbul, Turkey
关键词
fracture toughness; boronizing; alloy steels;
D O I
10.1016/S0257-8972(97)00466-0
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, we investigated the fracture toughness of boride layers formed on steel surfaces, The samples used for this study were prepared from low-alloy and low-carbon steels essentially containing Cr and/or Mn as the major elements, Boronizing was done in a salt bath consisting of borax, boric acid, and ferro-silicon. The temperature of the bath was 940 degrees C and the boronizing was conducted at an atmospheric pressure for 5-7 h. The presence of borides, e.g. Fe2B, was revealed by X-ray diffractometry, SEM, and optical microscopy. The fracture toughness of borided surfaces was measured via Vickers indenters with a load of 2 N. It was found that the fracture roughness of the borides ranged from 4 to 6 MPa m(1/2). The fracture toughness of the borides depends strongly on chemical composition of substrate and boronizing time. Mn as an alloying element has a beneficial effect on fracture toughness, and the longer boronizing time results in higher fracture toughness. (C) 1997 Elsevier Science S.A.
引用
收藏
页码:561 / 565
页数:5
相关论文
共 12 条
[1]  
Bindal C, 1996, APPL PHYS LETT, V68, P923, DOI 10.1063/1.116232
[2]  
BINDAL C, 1991, THESIS ISTANBUL TU I
[3]  
BINDAL C, 1991, P 1 INT S SCI ENG CE, P223
[4]  
COOK RF, 1983, COMMUN AM CERAM SOC, P200
[5]  
Cook SG, 1995, MATER SCI TECH SER, V11, P1093, DOI 10.1179/026708395790164490
[6]  
CUTLER RA, 1991, CERAMICS GLASSES, P787
[7]  
DAUTZENBERG N, 1979, POWDER METALL, P31
[8]   INDENTATION AND ACOUSTIC-EMISSION IN FILTRATION PROCESSED PLATELET REINFORCED CERAMICS [J].
FROM, PS ;
PYRZ, R ;
CLAUSEN, B ;
NIELSEN, EO .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 197 (02) :231-236
[9]   THE EFFECTS OF THIN COMPRESSIVE FILMS ON INDENTATION FRACTURE-TOUGHNESS MEASUREMENTS [J].
KOBRIN, PH ;
HARKER, AB .
JOURNAL OF MATERIALS SCIENCE, 1989, 24 (04) :1363-1367
[10]  
LAWN B, 1993, FRACTURE BRITTLE SOL, P257