Metal-support interactions in Pt/Al2O3 and Pd/Al2O3 catalysts for CO oxidation

被引:354
|
作者
Ivanova, A. S. [1 ]
Slavinskaya, E. M. [1 ]
Gulyaev, R. V. [1 ]
Zaikovskii, V. I. [1 ]
Stonkus, O. A. [2 ]
Danilova, I. G. [1 ]
Plyasova, L. M. [1 ]
Polukhina, I. A. [1 ]
Boronin, A. I. [1 ,2 ]
机构
[1] Boreskov Inst Catalysis SB RAS, Novosibirsk 630090, Russia
[2] Novosibirsk State Univ, Novosibirsk 630090, Russia
关键词
Supported catalysts; Alumina; Palladium; Platinum; CO oxidation; SMSI; HRTEM; XPS; TPR-H-2; Catalysis; SURFACE ELEMENTARY STEPS; RAY PHOTOELECTRON-SPECTROSCOPY; PALLADIUM-ALUMINA CATALYSTS; LOW-LOADED PALLADIUM; LIGHTING-OFF TESTS; INFRARED-SPECTROSCOPY; ELECTRON-MICROSCOPY; METHANE COMBUSTION; SILVER CATALYSTS; GAMMA-ALUMINA;
D O I
10.1016/j.apcatb.2010.03.024
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Platinum and palladium catalysts supported on gamma-Al203 were studied by XRD, UV-vis DRS, HRTEM. TPR-H-2, XPS together with measurements of their catalytic properties. The properties of the catalysts denoted as Pt(Pd)/Al2O3(X)-Y (X-the calcination temperature of support. degrees C. Y-the calcination temperciture of catalyst, C) were studied as a function of the temperatures used for calcination of the support and/or the catalyst in oxygen or in a reaction mixture of CO + O-2 It was found that the deposition of Pt or Pd on gamma-Al2O3 did not alter the structure of the support Two types of the Pt and Pd particles were typically present on the gamma-Al2O3 surface individual particles with dimensions of 1 5-3 nm and agglomerates about 100 nm in size In the catalysis calcined at relatively low temperatures (Pt/Al2O3(550)-450). platinum was present in the form of metal clusters However, in the Pd/Al2O3(550)-450 catalyst, the palladium particles were almost completely decorated with a thin layer of an alummate phase These structures are not reduced in hydrogen in the temperature range of -15 to 450 degrees C, and are stable to treatment in a reaction mixture of CO + O-2. Pd deposition on the gamma-Al2O3-800 support was found to result in stabilization of the active component in two main forms. Pd and PdO. with varying degrees of interaction due to the decoration effect Calcination at the low temperature of 550 degrees C led to the formation of a so-called "core-shell structure", where a palladium metal core is covered with a thin shell of an alummate phase Depending on the calcination temperature of the catalyst in the range of 450-1000 degrees C, the morphological form of the active component was converted from the "core-shell" state to a state consisting of two phases. Pd-o and PdO. with a gradual decrease of the Pd-o/PdO ratio, weakening the interaction with the support and the growth of palladium particles. Under the action of the reaction mixture, the Pd/Al2O3(800)-(450,600,800.1000) catalysts underwent changes in the Pd-o/PdO ratio, which regulates the light-off temperature After catalyst calcination at the highest temperature used in this study. 1200 degrees C. the palladium particles became much larger due to the loss of the palladium interaction with the support Only the metal phase of palladium was observed in these catalysts, and their catalytic activity decreases substantially. (C) 2010 Elsevier B.V All rights reserved
引用
收藏
页码:57 / 71
页数:15
相关论文
共 50 条
  • [31] The role of Pd precursors in the oxidation of carbon monoxide over Pd/Al2O3 and Pd/CeO2/Al2O3 catalysts
    Monteiro, RS
    Dieguez, LC
    Schmal, M
    CATALYSIS TODAY, 2001, 65 (01) : 77 - 89
  • [32] Oxidation of CO and Propane on Pt-Au/Al2O3 Catalysts
    Ruszel, M.
    Grzybowska-Swierkosz, B.
    Karpinski, Z.
    Juszczyk, W.
    POLISH JOURNAL OF CHEMISTRY, 2008, 82 (10) : 1991 - 1997
  • [33] Dynamics of Two-Step CO Oxidation Light-Off on Pt/-Al2O3 and Pd/-Al2O3 in the Presence of C3H6
    Brezina, Jan
    Boutikos, Panagiotis
    Arvajova, Adela Buzkova
    Pecinka, Rudolf
    Koci, Petr
    TOPICS IN CATALYSIS, 2019, 62 (1-4) : 252 - 258
  • [34] Investigation of Pt/γ-Al2O3 catalysts with locally high Pt concentrations for oxidation of CO at low temperatures
    Arnby, K
    Törncrona, A
    Andersson, B
    Skoglundh, M
    JOURNAL OF CATALYSIS, 2004, 221 (01) : 252 - 261
  • [35] Effect of phase composition between nano γ- and χ-Al2O3 on Pt/Al2O3 catalyst in CO oxidation
    Vleephoka, Chatchai
    Chaisuk, Choowong
    Samparnpiboon, Panida
    Praserthdam, Piyasan
    CATALYSIS COMMUNICATIONS, 2008, 9 (04) : 546 - 550
  • [36] High Catalytic Activity of Pt/Al2O3 Catalyst in CO Oxidation at Room Temperature-A New Insight into Strong Metal-Support Interactions
    Kocemba, Ireneusz
    Smiechowicz, Izabela
    Jedrzejczyk, Marcin
    Rogowski, Jacek
    Rynkowski, Jacek Michal
    CATALYSTS, 2021, 11 (12)
  • [37] Pt/Al2O3 with ultralow Pt-loading catalyze toluene oxidation: Promotional synergistic effect of Pt nanoparticles and Al2O3 support
    Gan, Tao
    Chu, Xuefeng
    Qi, Hui
    Zhang, Wenxiang
    Zou, Yongcun
    Yan, Wenfu
    Liu, Gang
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2019, 257
  • [38] Improvement of thermal stability of NO oxidation Pt/Al2O3 catalyst by addition of Pd
    Kaneeda, M.
    Iizuka, H.
    Hiratsuka, T.
    Shinotsuka, N.
    Arai, M.
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2009, 90 (3-4) : 564 - 569
  • [39] Influence of ammonia on CO and methanol oxidation over Pt/γ-Al2O3 catalysts modified by Mg
    Arnby, K
    Törncrona, A
    Skoglundh, M
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2004, 49 (01) : 51 - 59
  • [40] A transient in situ FTIR and XANES study of CO oxidation over Pt/Al2O3 catalysts
    Carlsson, PA
    Österlund, L
    Thormählen, P
    Palmqvist, A
    Fridell, E
    Jansson, J
    Skoglundh, M
    JOURNAL OF CATALYSIS, 2004, 226 (02) : 422 - 434