Metal-support interactions in Pt/Al2O3 and Pd/Al2O3 catalysts for CO oxidation

被引:354
|
作者
Ivanova, A. S. [1 ]
Slavinskaya, E. M. [1 ]
Gulyaev, R. V. [1 ]
Zaikovskii, V. I. [1 ]
Stonkus, O. A. [2 ]
Danilova, I. G. [1 ]
Plyasova, L. M. [1 ]
Polukhina, I. A. [1 ]
Boronin, A. I. [1 ,2 ]
机构
[1] Boreskov Inst Catalysis SB RAS, Novosibirsk 630090, Russia
[2] Novosibirsk State Univ, Novosibirsk 630090, Russia
关键词
Supported catalysts; Alumina; Palladium; Platinum; CO oxidation; SMSI; HRTEM; XPS; TPR-H-2; Catalysis; SURFACE ELEMENTARY STEPS; RAY PHOTOELECTRON-SPECTROSCOPY; PALLADIUM-ALUMINA CATALYSTS; LOW-LOADED PALLADIUM; LIGHTING-OFF TESTS; INFRARED-SPECTROSCOPY; ELECTRON-MICROSCOPY; METHANE COMBUSTION; SILVER CATALYSTS; GAMMA-ALUMINA;
D O I
10.1016/j.apcatb.2010.03.024
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Platinum and palladium catalysts supported on gamma-Al203 were studied by XRD, UV-vis DRS, HRTEM. TPR-H-2, XPS together with measurements of their catalytic properties. The properties of the catalysts denoted as Pt(Pd)/Al2O3(X)-Y (X-the calcination temperature of support. degrees C. Y-the calcination temperciture of catalyst, C) were studied as a function of the temperatures used for calcination of the support and/or the catalyst in oxygen or in a reaction mixture of CO + O-2 It was found that the deposition of Pt or Pd on gamma-Al2O3 did not alter the structure of the support Two types of the Pt and Pd particles were typically present on the gamma-Al2O3 surface individual particles with dimensions of 1 5-3 nm and agglomerates about 100 nm in size In the catalysis calcined at relatively low temperatures (Pt/Al2O3(550)-450). platinum was present in the form of metal clusters However, in the Pd/Al2O3(550)-450 catalyst, the palladium particles were almost completely decorated with a thin layer of an alummate phase These structures are not reduced in hydrogen in the temperature range of -15 to 450 degrees C, and are stable to treatment in a reaction mixture of CO + O-2. Pd deposition on the gamma-Al2O3-800 support was found to result in stabilization of the active component in two main forms. Pd and PdO. with varying degrees of interaction due to the decoration effect Calcination at the low temperature of 550 degrees C led to the formation of a so-called "core-shell structure", where a palladium metal core is covered with a thin shell of an alummate phase Depending on the calcination temperature of the catalyst in the range of 450-1000 degrees C, the morphological form of the active component was converted from the "core-shell" state to a state consisting of two phases. Pd-o and PdO. with a gradual decrease of the Pd-o/PdO ratio, weakening the interaction with the support and the growth of palladium particles. Under the action of the reaction mixture, the Pd/Al2O3(800)-(450,600,800.1000) catalysts underwent changes in the Pd-o/PdO ratio, which regulates the light-off temperature After catalyst calcination at the highest temperature used in this study. 1200 degrees C. the palladium particles became much larger due to the loss of the palladium interaction with the support Only the metal phase of palladium was observed in these catalysts, and their catalytic activity decreases substantially. (C) 2010 Elsevier B.V All rights reserved
引用
收藏
页码:57 / 71
页数:15
相关论文
共 50 条
  • [21] MICROCALORIMETRIC AND DEHYDROGENATION ACTIVITY STUDIES OF Pt/γ-Al2O3 AND Pt-Sn/γ-Al2O3 CATALYSTS
    Jia Jifei 1
    2 Department of Chemistry
    催化学报, 1997, (01) : 2 - 3
  • [22] Reactivation of sintered Pt/Al2O3 oxidation catalysts
    Galisteo, FC
    Mariscal, R
    Granados, ML
    Fierro, JLG
    Daley, RA
    Anderson, JA
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2005, 59 (3-4) : 227 - 233
  • [23] Electrochemically Synthesized Pt/Al2O3 Oxidation Catalysts
    Dmitry E. Doronkin
    Aleksandra B. Kuriganova
    Igor N. Leontyev
    Sina Baier
    Henning Lichtenberg
    Nina V. Smirnova
    Jan-Dierk Grunwaldt
    Catalysis Letters, 2016, 146 : 452 - 463
  • [24] Hydrodesulfurization of coal tar pitch using Pt/Al2O3 and Pd/Al2O3 catalysts under mild conditions
    Yazu, Kazumasa
    Sharma, Atul
    CARBON RESOURCES CONVERSION, 2019, 2 (03): : 213 - 216
  • [25] Effect of metal-support interactions in Ni/Al2O3 catalysts with low metal loading for methane dry reforming
    Ewbank, Jessica L.
    Kovarik, Libor
    Diallo, Fatoumata Z.
    Sievers, Carsten
    APPLIED CATALYSIS A-GENERAL, 2015, 494 : 57 - 67
  • [26] Catalytic oxidation of CO by O-2 on NiO/Al2O3 catalysts
    ElShobaky, GA
    Hassan, HA
    Ahmad, AS
    AFINIDAD, 1997, 54 (471) : 382 - 386
  • [27] CO Oxidation on Pd/Al2O3 Catalysts under Stoichiometric Conditions
    Dai Quy Phan
    Sven Kureti
    Topics in Catalysis, 2017, 60 : 260 - 265
  • [28] Metal Support Interactions in Co3O4/Al2O3 Catalysts Prepared from w/o Microemulsions
    Fischer, N.
    Minnermann, M.
    Baeumer, M.
    van Steen, E.
    Claeys, M.
    CATALYSIS LETTERS, 2012, 142 (07) : 830 - 837
  • [29] Methane combustion over Pd/γ-Al2O3 and Pd-VOx/γ-Al2O3 catalysts
    Neyertz, C
    Volpe, M
    Gigola, C
    APPLIED CATALYSIS A-GENERAL, 2004, 277 (1-2) : 137 - 145
  • [30] Selective ring opening of methylcyclopentane over Pt/γ-Al2O3, Ir/γ-Al2O3 and Pt-Ir/γ-Al2O3 catalysts with hydrogen at atmospheric pressure
    Djeddi, Amel
    Fechete, Ioana
    Garin, Francois
    APPLIED CATALYSIS A-GENERAL, 2012, 413 : 340 - 349