Wear properties of dental ceramics and porcelains compared with human enamel

被引:91
作者
D'Arcangelo, Camillo [1 ]
Vanini, Lorenzo
Rondoni, Giuseppe D.
De Angelis, Francesco [1 ]
机构
[1] Univ G dAnnunzio, Sch Dent, Dept Restorat Dent, I-66100 Chieti, Italy
关键词
RESIN DENTURE TEETH; NANOFILLED COMPOSITE RESIN; IN-VITRO WEAR; RESTORATIVE MATERIALS; FLEXURAL STRENGTH; ARTIFICIAL TEETH; TOOTH WEAR; GOLD; RESISTANCE; ANTAGONIST;
D O I
10.1016/j.prosdent.2015.09.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. Contemporary pressable and computer-aided design/manufacturing (CAD/CAM) ceramics exhibit good mechanical and esthetic properties. Their wear resistance compared with human enamel and traditional gold based alloys needs to be better investigated. Purpose. The purpose of this in vitro study was to compare the 2-body wear resistance of human enamel, gold alloy, and 5 different dental ceramics, including a recently introduced zirconia-reinforced lithium silicate ceramic (Celtra Duo). Material and methods. Cylindrical specimens were fabricated from a Type III gold alloy (Aurocast8), 2 hot pressed ceramics (Imagine PressX, IPS e.max Press), 2 CAD/CAM ceramics (IPS e.max CAD, Celtra Duo), and a CAD/CAM feldspathic porcelain (Vitablocs Mark II) (n=10). Celtra Duo was tested both soon after grinding and after a subsequent glaze firing cycle. Ten flat human enamel specimens were used as the control group. All specimens were subjected to a 2-body wear test in a dual axis mastication simulator for 120 000 loading cycles against yttria stabilized tetragonal zirconia polycrystal cusps. The wear resistance was analyzed by measuring the vertical substance loss (mm) and the volume loss (mm(3)). Antagonist wear (mm) was also recorded. Data were statistically analyzed with 1-way ANOVA tests (alpha=.05). Results. The wear depth (0.223 mm) of gold alloy was the closest to that of human enamel (0.217 mm), with no significant difference (P>.05). The greatest wear was recorded on the milled Celtra Duo (wear depth=0.320 mm), which appeared significantly less wear resistant than gold alloy or human enamel (P<.05). Conclusions. The milled and not glazed Celtra Duo showed a small but significantly increased wear depth compared with Aurocast8 and human enamel. Wear depth and volumetric loss for the glaze-fired Celtra Duo and for the other tested ceramics did not statistically differ in comparison with the human enamel.
引用
收藏
页码:350 / 355
页数:6
相关论文
共 52 条
  • [1] An Investigation into the Role of Core Porcelain Thickness and Lamination in Determining the Flexural Strength of In-Ceram Dental Materials
    Alshehri, Sharifa Abdullah
    [J]. JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2011, 20 (04): : 261 - 266
  • [2] THREE-BODY WEAR POTENTIAL OF DENTAL YTTRIUM-STABILIZED ZIRCONIA CERAMIC AFTER GRINDING, POLISHING, AND GLAZING TREATMENTS
    Amer, Rafat
    Kurklu, Duygu
    Kateeb, Elham
    Seghi, Robert R.
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2014, 112 (05) : 1151 - 1155
  • [3] Barco M T Jr, 1989, Int J Prosthodont, V2, P365
  • [4] Abrasionen oberer und unterer frontzähne in relation zur inzisalen und kondylären führungWear in the upper and lower incisors in relation to incisal and condylar guidance
    W. Bauer
    F. van den Hoven
    P. Diedrich
    [J]. Journal of Orofacial Orthopedics / Fortschritte der Kieferorthopädie, 1997, 58 (6): : 306 - 319
  • [5] Fracture behavior of lithia disilicate- and leucite-based ceramics
    Bona, AD
    Mecholsky, JJ
    Anusavice, KJ
    [J]. DENTAL MATERIALS, 2004, 20 (10) : 956 - 962
  • [6] Burke F J Trevor, 2002, J Adhes Dent, V4, P7
  • [7] In vitro wear of composite with varied cure, filler level, and filler treatment
    Condon, JR
    Ferracane, JL
    [J]. JOURNAL OF DENTAL RESEARCH, 1997, 76 (07) : 1405 - 1411
  • [8] Wear Properties of a Novel Resin Composite Compared to Human Enamel and Other Restorative Materials
    D'Arcangelo, C.
    Vanini, L.
    Rondoni, G. D.
    Pirani, M.
    Vadini, M.
    Gattone, M.
    De Angelis, F.
    [J]. OPERATIVE DENTISTRY, 2014, 39 (06) : 612 - 618
  • [9] The Influence of Luting Systems on the Microtensile Bond Strength of Dentin to Indirect Resin-based Composite and Ceramic Restorations
    D'Arcangelo, C.
    De Angelis, F.
    D'Amario, M.
    Zazzeroni, S.
    Ciampoli, C.
    Caputi, S.
    [J]. OPERATIVE DENTISTRY, 2009, 34 (03) : 328 - 336
  • [10] Fracture Resistance and Deflection of Pulpless Anterior Teeth Restored with Composite or Porcelain Veneers
    D'Arcangelo, Camillo
    De Angelis, Francesco
    Vadini, Mirco
    D'Amario, Maurizio
    Caputi, Sergio
    [J]. JOURNAL OF ENDODONTICS, 2010, 36 (01) : 153 - 156