Increase in Adhesion Strength and Thickness of Cubic Boron Nitride Thin Films by Silicon Addition

被引:0
|
作者
Ohori, Tetsutaro [1 ]
Shirahata, Jun [1 ]
Asami, Hiroki [1 ]
Suzuki, Tsuneo [1 ]
Nakayama, Tadachika [1 ]
Suematsu, Hisayuki [1 ]
Niihara, Koichi [1 ]
机构
[1] Nagaoka Univ Technol, Extreme Energy Dent Res Inst, Nagoaka 9402188, Japan
关键词
cubic boron nitride; silicon addition; radio frequency magnetron sputtering; combinatorial method; hardness; IMPROVEMENT; DEPOSITION;
D O I
10.2320/jinstmet.74.36
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Compositionally gradient boron nitride with silicon (BN:Si) thin films have been prepared on silicon (100) substrates by radio frequency magnetron sputtering. A hexagonal boron nitride (h-BN) target with uneven distribution of silicon plates was used for the deposition. The present study was focused on the investigation of the morphology, the microstructure, the determination of silicon composition, the bonding structure and the micro-hardness using scanning electron microscopy (SEAM), Rutherford back scattering spectroscopy (RBS), Fourier transform infra-red spectroscopy (FT-IR) and micro-hardness testing with a Vickers indenter. The BN:Si thin films with the thicknesses of 100 similar to 850 run were not peeled off as compared to the boron nitride thin films with the same thicknesses. Increasing the Si content of the boron nitride thin films induced a decrease in fraction of spa bonding. The cubic boron nitride (c-BN) thin film with silicon addition was deposited with a thickness of 850 nm at 5.2 mol% silicon content. On the other hand, the hardness was 72 GPa and the young's modulus was 286 GPa. Since the c-BN:Si thin film was peeled off from silicon substrate at a few weeks after the deposition, compressive stress was not completely released by silicon addition.
引用
收藏
页码:36 / 41
页数:6
相关论文
共 50 条
  • [1] Nucleation of cubic boron nitride thin films
    Collazo-Davila, C
    Bengu, E
    Marks, LD
    Kirk, M
    DIAMOND AND RELATED MATERIALS, 1999, 8 (06) : 1091 - 1100
  • [2] Synthesis of cubic boron nitride thin films
    McKenzie, DR
    McFall, WD
    Reisch, S
    James, BW
    Falconer, IS
    Boswell, RW
    Persing, H
    Perry, AJ
    Durandet, A
    SURFACE & COATINGS TECHNOLOGY, 1996, 78 (1-3) : 255 - 262
  • [3] Deposition of cubic boron nitride thin films by IBED
    Kuang, YZ
    Huang, XG
    You, DW
    Wang, XM
    Lin, WL
    MATERIALS CHEMISTRY AND PHYSICS, 1998, 53 (03) : 267 - 270
  • [4] Surface properties of cubic boron nitride thin films
    Deng, Jinxiang
    Chen, Guanghua
    APPLIED SURFACE SCIENCE, 2006, 252 (22) : 7766 - 7770
  • [5] Adhesion improvement of cubic boron nitride films by in situ annealing
    Yu, J
    Song, SH
    Weng, LQ
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (16-17) : 4737 - 4740
  • [6] Stress reduction of cubic boron nitride films by oxygen addition
    Ye, J.
    Ulrich, S.
    Zlebert, C.
    Stueber, M.
    THIN SOLID FILMS, 2008, 517 (03) : 1151 - 1155
  • [7] Effects of silicon incorporation on composition, structure and electric conductivity of cubic boron nitride thin films
    Ying, J.
    Zhang, X. W.
    Fan, Y. M.
    Tan, H. R.
    Yin, Z. G.
    DIAMOND AND RELATED MATERIALS, 2010, 19 (11) : 1371 - 1376
  • [8] Synthesis of cubic boron nitride thin films on silicon substrate using electron beam evaporation
    Nasrazadani, S
    Vemuri, P
    Characterization and Metrology for ULSI Technology 2005, 2005, 788 : 501 - 506
  • [9] Microstructure and stress investigations of cubic boron nitride thin films
    Ilias, S
    Stambouli, V
    Pascallon, J
    Bouchier, D
    Nouet, G
    DIAMOND AND RELATED MATERIALS, 1998, 7 (2-5) : 391 - 396
  • [10] Improvement of the adhesion of cubic boron nitride films by adding miscellaneous elements
    Kurooka, S
    Ikeda, T
    Tanaka, A
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2003, 206 : 1088 - 1091